Stainless Steel 316Ti Pipes & Tubes
ASTM A269 TP 316TI SS Seamless Pipes, SS ASTM A312 TP 316TI Round Tubes, TP 316TI SS Polished Pipes, Stainless Steel 316TI Black Round Tubes, TP 316TI SS ERW Pipes Exporter, Manufacturer in Mumbai,India.
Nickel Super Alloys is one of the leading distributor, exporter and supplier of Stainless Steel 316Ti Pipes and Tubes, which exists as the preferred material in many specifications. A heat treatment after welding for Stainless Steel 316Ti Seamless Pipes is normally not used. Stainless Steel 316Ti Welded Tubes is found to be more applicable in areas with high or elevated temperatures compared to other alloys. Stainless Steel 316Ti EFW Pipes is suited to use in heavygauge welded components. Corrosion resistance is improved in Stainless Steel 316Ti Round Tubes, particularly against sulfuric and hydrochloric acids. Stainless Steel 316Ti Square Pipes contains high nickel content and a high amount of chromium. Post-weld annealing for Stainless Steel 316Ti Rectangular Tubes is not required when welding thin sections.
For outdoor furnishings like rails and bollards, Stainless Steel 316Ti ERW Pipes is an ideal corrosion-resistant material. Stainless Steel 316Ti Hexagonal Tubes are non-hardenable by heat treatment and can be readily formed and drawn. Stainless Steel 316Ti Electropolish Pipes does not suffer uniform corrosion, like carbon steel, when exposed to wet environments. Stainless Steel 316Ti Bush Hex Tubeshardens rapidly during mechanical working. Stainless Steel 316Ti Hallow Pipes possesses excellent mechanical and corrosion properties at sub-zero temperatures. Stainless Steel UNS S31609 Tubes has an outstanding formability and weldability. 316Ti Stainless Steel Pipes is often used in oil & petroleum refining equipment. 316Ti Stainless Steel Tubes finds limited applications due to their poor mechanical properties and due to the presence of porosity.
ASTM A213 SS 316TI Pipes, SS DIN 1.4571 Rectangular Welded Tubes, ASTM A312 SS TP 316TI Seamless Pipes, Stainless Steel 316TI Welded Tubes, SS UNS S31609 Square Pipes, 316TI Stainless Steel EFW Tubing Suppliers in India.
Key Charactristic:
- Corrosion resistance
- Resistance to oxidation and sulfidation
- Cryogenic strength
- Resistance to abrasion and erosion
- Surface finish
- Magnetic properties
- Ductility
- Elevated temperature strength
- Stability of properties in service
- Suitability for intended fabrication techniques
SS 316Ti Pipe Stock Size Range and Specifications
| Grade | Stainless Steel 316Ti / SS TP 316Ti / DIN 1.4571 Pipes / UNS S31635 Pipes |
| Size | 1/2" NB - 24" NB |
| Standard | ASTM / ASME SA213 / A249 / A269 / A312 / A358 CL. I to V ASTM A789 / A790 |
| Steel EFW 316Ti Pipes | 6" NB - 100" NB |
| Form | Round, Square, Rectangular, Hydraulic Etc |
| Schedule | SCH20, SCH30, SCH40, STD, SCH80, XS, SCH60, SCH80, SCH120, SCH140, SCH160, XXS |
| Length | Single Random, Double Random & Cut Length. (Custom Sizes Available as per customers requirement) |
| Type | Seamless / ERW / Welded / Fabricated / EFW |
| End | Plain End, Beveled End, Treaded |
| Standard | SS 316TI |
| Werkstoff Nr. | 1.4571 |
| UNS | S31635 |
| JIS | SUS 316Ti |
| AFNOR | Z6CNDT17-12 |
| BS | 320S31 |
| GOST | 08Ch17N13M2T |
| EN | X6CrNiMoTi17-12-2 |
316Ti Stainless Steel Pipes Chemical Composition
| Grade | C | Mn | Si | P | S | Cr | Mo | Ni | N | |
| 316Ti | min. | – | – | – | – | – | 16.0 | 2.00 | 10.0 | – |
| max. | 0.08 | 2.0 | 0.75 | 0.045 | 0.030 | 18.0 | 3.00 | 14.0 | – | |
Stainless Steel 316Ti Pipe Mechanical Properties
| Grade | Tensile Strength (MPa) min | Yield Strength 0.2% Proof (MPa) min | Elongation (% in 50mm) min | Hardness | |
| Rockwell B (HR B) max | Brinell (HB) max | ||||
| 316Ti | 515 | 205 | 35 | 75 | 205 |
Other Types of Stainless Steel 316Ti Pipes & Stainless Steel Tubes
- SS 316Ti Seamless Pipes Supplier in UAE
- Stainless Steel 316Ti Pipes Manufacturer in India
- SS 316Ti Welded Pipes
- ASTM A312 TP 316Ti Fabricated Pipes
- Stainless Steel 316Ti Tubes
- SS 316Ti Round Tubes
- Stainless Steel 316Ti Square Pipe
- 316Ti Electropolish ERW Pipes
- UNS S31635 Hexagonal Pipe
- 316Ti Stainless Stel Hallow Pipe
- UNS S31635 Welded Tubes Exporter in Russia
- Steel 316Ti Bush Hex Pipe
- Stainless Steel 316Ti Round Pipe Supplier in Poland
- SS 316Ti ERW Pipes
- Stainless Steel 316Ti EFW Pipes in Qatar
- DIN 1.4571 Steel Pipes
- Werkstoff Nr. 1.4571 Steel Tubes
- X6CrNiMoTi17-12-2 Pipes
- SUS 316Ti Pipes
- SUS 316Ti Rectangular Pipe
Countries We Export to
Nickel Super Alloys manufactures and exports Stainless Steel 316Ti Pipes to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia
Cities We Deliver to
Nickel Super Alloys manufactures and exports Stainless Steel 316Ti Pipes to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo