Stainless Steel 310 / 310S Pipes & Tubes
ASTM A312 Stainless Steel 310 Pipe & Tubes, SS UNS S31008 Welded Pipe & Tubes, 310s SS Hexagonal Pipe & Tubes, Stainless Steel WERKSTOFF NR. 1.4841 Pipe & Tubes Manufacturer in Mumbai,India.
Nickel Super Alloys is a prominent firm in manufacturing an exporting Stainless Steel 310 / 310S Pipes and Tubes, which is a high temperature chromium nickel austenitic stainless steel. Stainless Steel 310 Seamless Pipes is used for construction parts which should be resistant to scaling up to about 1050 Degree C. Stainless Steel 310S Welded Tubes is austenitic heat resisting steel with very good oxidation resistance. Stainless Steel 310 EFW Pipes are typically used for elevated temperature applications. An austenitic chromium-nickel grade, Stainless Steel 310S ERW Tubes displays excellent oxidation resistance up to 1094 Degree C. Stainless Steel 310 Round Pipes has excellent resistance to oxidation under mildly cyclic conditions through 2000 Degree F. Stainless Steel 310S Square Tubes is developed for use in high temperature corrosion resistant applications.
Stainless Steel 310 Rectangular Pipes is used for high temperature applications such as furnace parts and heat treatment equipment. Stainless Steel 310S Electropolish Tubes combines excellent high temperature properties with good ductility and weldability. Stainless Steel 310 Hexagonal Pipes is suggested for applications where sensitization and subsequent corrosion by high temperature gases or condensates during shutdown may pose a problem. Stainless Steel 310S Bush Hex Tubes has high chromium and medium nickel contents. Stainless Steel UNS S31000 Pipes is one of the most widely used grades of heat resistant stainless steel supplied into numerous industry sectors. Stainless Steel UNS S31008 Tubes has carbon content and is a preferred choice for high temperature applications.
310 – 310S SS Seamless Pipes & Tubes, Stainless Steel 310 Seamless Pipe & Tubes, Stainless Steel 310S Welded Pipes & Tubes, ASTM A312 TP 310 – 310S SS Electropolished Pipes & Tubes, SS UNS S31000 Welded Pipe & Tubes Suppliers in India.
Key Charactristic:
- Corrosion resistance
- Resistance to oxidation and sulfidation
- Cryogenic strength
- Resistance to abrasion and erosion
- Surface finish
- Magnetic properties
- Ductility
- Elevated temperature strength
- Stability of properties in service
- Suitability for intended fabrication techniques
SS 310 / 310s Pipe Stock Size Range and Specifications
| Grade | SS 310 / TP 310 Stainless Steel Pipes / Stainless Steel 310S / TP 310S Stainless Steel Pipes |
| Size | 1/8″NB TO 30″NB IN |
| Standard | ASTM A / ASME SA213 / A249 / A269 / A312 / A358 CL. I to V |
| Form | Round Pipes, Square Pipes, Rectangular Pipe, “U” Shape, Oval Pipes, Hydraulic Pipes |
| Schedule | SCH 5, SCH10, SCH 40, SCH 80, SCH 80S, SCH 160, SCH XXS, SCH XS |
| Length | Single Random, Double Random & Cut Length. |
| Type | Seamless / ERW / Welded / Fabricated / EFW /LSAW |
| End | Plain End, Beveled End, Treaded |
| Standard | SS 310 | SS 310S |
| UNS | S31000 | S31008 |
| WERKSTOFF NR. | 1.4841 | 1.4845 |
| AFNOR | - | - |
| JIS | - | - |
| GOST | - | - |
| BS | - | - |
| EN | - | - |
310 / 310S Stainless Steel Pipes Chemical Composition
| Grade | C | Mn | Si | P | S | Cr | Mo | Ni | N | |
| 310 |
min. | – | – | – | – | – | 24.0 | – | 19.0 | – |
| max. | 0.25 | 2.0 | 1.50 | 0.045 | 0.030 | 26.0 | 22.0 | – | ||
Stainless Steel 310 / 310s Pipe Mechanical Properties
| Grade | Tensile Strength (MPa) min | Yield Strength 0.2% Proof (MPa) min | Elongation (% in 50mm) min | Hardness | |
| Rockwell B (HR B) max | Brinell (HB) max | ||||
| 310 – 310S | 515 | 205 | 40 | 95 | 217 |
Other Types of Stainless Steel 310 / 310S Pipes & Stainless Steel Tubes
- SS 310 Seamless Pipes Supplier in UAE
- Stainless Steel 310s Pipes Manufacturer in India
- SS 310 Welded Pipes
- ASTM A312 TP 310s Fabricated Pipes
- Stainless Steel 310 Tubes
- SS 310s Round Tubes
- Stainless Steel 310 Square Pipe
- 310s Electropolish ERW Pipes
- UNS S31000 / S31008 Hexagonal Pipe
- 310 Stainless Stel Hallow Pipe
- UNS S31000 / S31008 Welded Tubes Exporter in Russia
- Steel 310s Bush Hex Pipe
- Stainless Steel 310 Round Pipe Supplier in Poland
- SS 310s ERW Pipes
- Stainless Steel 310 EFW Pipes in Qatar
- DIN 1.4841 / 1.4845 Steel Pipes
- Werkstoff Nr. 1.4841 / 1.4845 Steel Tubes
- Stainless Steel 310 Tubing
- SUS 310s Pipes
- SUS 310 Rectangular Pipe
Countries We Export to
Nickel Super Alloys manufactures and exports Stainless Steel 310 / 310s Pipes to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia
Cities We Deliver to
Nickel Super Alloys manufactures and exports Stainless Steel 310 / 310s Pipes to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo