Stainless Steel 304 Pipes & Tubes
Stainless Steel WERKSTOFF NR. 1.4301 Pipe & Tubes, ASTM A312 Stainless Steel Pipe & Tubes, SS 304 Hexagonal Pipe & Tubes, Austenitic Stainless Steel 304 Pipes & Tubes Manufacturer in Mumbai,India.
Nickel Super Alloys is one of leading supplier and distributor of Stainless Steel 304 Pipes and Tubes, which has a minimum of 18 percent of chromium and 8 percent of nickel in it. Stainless Steel 304 Seamless Pipes contains a higher chromium and lower carbon content than other variations. Stainless Steel 304 Welded Tube sare comprised of at least 10 percent chromium and have better corrosion resistance properties. Stainless Steel 304 EFW Pipes is an austenitic grade that can be severely deep drawn. Stainless Steel 304 ERW Tubeshas ability to resist rusting thanks to the interaction between its alloying components and the environment to which they're exposed.
Stainless Steel 304 Round Pipes is held in a temperature range 450 Degree C to 850 Degree C for periods of several minutes. Stainless Steel 304 Square Tubes represents between 50 percent- 60 percent of consumption of stainless materials and fins applications in almost every industry. Stainless Steel 304 Rectangular Pipes may be susceptible to inter-granular corrosion in certain corrosive media. Stainless Steel 304 Electropolish Tubes exhibit excellent corrosion resistance to a wide range of corrosive environments. Stainless Steel 304 Hexagonal Pipes has typical values for specimens of unknown form/heat treatment but appear to be annealed samples. Non-magnetic Stainless Steel UNS S30400 Tubes is the most versatile and the most widely used of all stainless steels.
304 Stainless Steel Seamless Pipes & Tubes, ASTM A312 TP 304 Stainless Steel Seamless Pipes & Tubes, 304 SS Electropolished Pipes & Tubes,304 SS Hallow Pipe & Tubes, SS UNS S30400 Welded Pipe & Tubes Suppliers in India.
Key Charactristic:
- Corrosion resistance
- Resistance to oxidation and sulfidation
- Cryogenic strength
- Resistance to abrasion and erosion
- Surface finish
- Magnetic properties
- Ductility
- Elevated temperature strength
- Stability of properties in service
- Suitability for intended fabrication techniques
SS 304 Pipe Stock Size Range and Specifications
| Grade | Stainless Steel 304 |
| Size | 1/8″NB TO 30″NB IN |
| Standard | ASTM / ASME SA312 / A249 / A269 / A312 / A358 CL. I to V ASTM A789/A790 |
| Steel 304 Pipes | 1/2" NB - 16" NB |
| Form | Round, Square, Rectangular, Hydraulic Etc |
| Schedule | SCH20, SCH30, SCH40, STD, SCH80, XS, SCH60, SCH80, SCH120, SCH140, SCH160, XXS |
| Length | Single Random, Double Random & Cut Length. |
| Type | Seamless / ERW / Welded / Fabricated / EFW |
| End | Plain End, Beveled End, Treaded |
| Standard | SS 304 |
| Werkstoff Nr. | 1.4301 |
| UNS | S30400 |
| JIS | SUS 304 |
| AFNOR | Z7CN18‐09 |
| BS | 304S31 |
| GOST | 08Х18Н10 |
| EN | X5CrNi18-10 |
304 Stainless Steel Pipes Chemical Composition
| Grade | C | Mn | Si | P | S | Cr | Mo | Ni | N | |
| 304 | min. | – | – | – | – | – | 18.0 | – | 8.0 | – |
| max. | 0.08 | 2.0 | 0.75 | 0.045 | 0.030 | 20.0 | 10.5 | 0.10 | ||
Stainless Steel 304 Pipe Mechanical Properties
| Grade | Tensile Strength (MPa) min | Yield Strength 0.2% Proof (MPa) min | Elongation (% in 50mm) min | Hardness | |
| Rockwell B (HR B) max | Brinell (HB) max | ||||
| 304 | 515 | 205 | 40 | 92 | 201 |
Other Types of Stainless Steel Pipes & Stainless Steel Tubes
- SS 304 Seamless Pipes Supplier in UAE
- Stainless Steel 304 Pipes Manufacturer in India
- SS 304 Welded Pipes
- ASTM A312 TP 304 304 Fabricated Pipes
- Stainless Steel 304 Tubes
- SS 304 Round Tubes
- Stainless Steel 304 Square Pipe
- 304 Electropolish ERW Pipes
- UNS S30400 Hexagonal Pipe
- 304 Stainless Stel Hallow Pipe
- UNS S30400 Welded Tubes Exporter in Russia
- Steel 304 Bush Hex Pipe
- Stainless Steel 304 Round Pipe Supplier in Poland
- SS 304 ERW Pipes
- Stainless Steel 304 EFW Pipes in Qatar
- DIN 1.4301 Steel Pipes
- Werkstoff Nr. 1.4301 Steel Tubes
- EN X5CrNi18-10 Pipes
- SUS 304 Pipes
- SUS 304 Rectangular Pipe
Countries We Export to
Nickel Super Alloys manufactures and exports Stainless Steel 304 Pipes to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia
Cities We Deliver to
Nickel Super Alloys manufactures and exports Stainless Steel 304 Pipes to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo