Stainless Steel 304L Pipes & Tubes
SS DIN 1.4306/1.4307 Rectangular Welded Pipes, TP 304L SS ERW Pipes, Stainless Steel 304L Black Round Tubes, Stainless Steel 304L Welded Tubes, 304L Stainless Steel EFW Tubing, Manufacturer in Mumbai,India.
Nickel Super Alloys is one of leading distributor and supplier of Stainless Steel 304L Pipes and Tubes, which is one of the most versatile and commonly used stainless steels in the market. An understanding of the attributes of Stainless Steel 304L Seamless Pipes provides an excellent base for comparing members of the austenitic family of stainless steels. Stainless Steel 304L Welded Tubes contains both chromium (between 18 percent –20 percent) and nickel (between 8 percent –10.5 percent)metals as the main non-iron constituents. Stainless Steel 304L EFW Pipes has a minimum of chromium and nickel, combined with a maximum of carbon.
Stainless Steel 304L ERW Tubes stains less easily than other iron-based metals. When selecting a stainless steel that must endure corrosive environments, austenitic Stainless Steel 304L Round Pipes are typically used. The molybdenum in Stainless Steel 304L Square Tubes is added to help resist corrosion to chlorides (like sea water and de-icing salts). The chemical composition, weldability, mechanical properties, and corrosion/oxidation resistance of Stainless Steel 304L Rectangular Pipes provide the best all-round performance stainless steel at relatively low cost. Stainless Steel 304L Electropolish Tubes is available in a wider range of products, finishes and forms than any other. Stainless Steel 304L Hexagonal Pipes is an austenitic grade that can be severely deep drawn. Stainless Steel UNS S30403 Tubes refers to its durability, quality, and temperature resistance.
ASTM A213, A312 SS Seamless Pipes, UNS S30403 Square Pipes, ASTM A312 TP 304L SS Seamless Pipes Manufacturer, ASTM A213 304L Round Pipes, 304L Polished Pipes, ASTM A249 304L Pipes Suppliers in India.
Key Charactristic:
- Corrosion resistance
- Resistance to oxidation and sulfidation
- Cryogenic strength
- Resistance to abrasion and erosion
- Surface finish
- Magnetic properties
- Ductility
- Elevated temperature strength
- Stability of properties in service
- Suitability for intended fabrication techniques
SS 304L Pipe Stock Size Range and Specifications
| Grade | TP 304L Stainless Steel Pipes / UNS S30403 / DIN 1.4306 / 1.4307 |
| Size | 1/2" NB to 24" NB |
| Standard | ASTM A249/ A269 / A312 / A358 / A409 / A554 / A778 / A789 / A790 |
| Form | Round Pipes, Square Pipes, Rectangular Pipes, Oval Pipes, Hydraulic Pipe, etc. |
| Schedule | SCH20, SCH30, SCH40, STD, SCH80, XS, SCH60, SCH80, SCH120, SCH140, SCH160, XXS |
| Length | Single Random, Double Random & Cut Length. |
| Type | Seamless / ERW / Welded / Fabricated / LSAW / EFW |
| End | Plain End, Beveled End, Treaded |
| Standard | SS 304L |
| Werkstoff Nr. | 1.4306 / 1.4307 |
| UNS | S30403 |
| JIS | SUS 304L |
| AFNOR | Z3CN18-10 |
| BS | 304S11 |
| GOST | 03Х18Н11 |
| EN | X2CrNi18-9 / X2CrNi19-11 |
304L Stainless Steel Pipes Chemical Composition
| Grade | C | Mn | Si | P | S | Cr | Mo | Ni | N | |
| 304L | min. | – | – | – | – | – | 18.0 | – | 8.0 | – |
| max. | 0.03 | 2.0 | 1.00 | 0.045 | 0.03 | 20.0 | 12.0 | – | ||
Stainless Steel 304L Pipe Mechanical Properties
| Grade | Tensile Strength (MPa) min | Yield Strength 0.2% Proof (MPa) min | Elongation (% in 50mm) min | Hardness | |
| Rockwell B (HR B) max | Brinell (HB) max | ||||
| 304L | 485 | 170 | 40 | 92 | 201 |
Other Types of Stainless Steel 304L Pipes & Stainless Steel Tubes
- SS 304L Seamless Pipes Supplier in UAE
- Stainless Steel 304L Pipes Manufacturer in India
- SS 304L Welded Pipes
- ASTM A312 TP 304L Fabricated Pipes
- Stainless Steel 304L Tubes
- SS 304L Round Tubes
- Stainless Steel 304L Square Pipe
- 304L Electropolish ERW Pipes
- UNS S30403 Hexagonal Pipe
- 304L Stainless Stel Hallow Pipe
- UNS S30403 Welded Tubes Exporter in Russia
- Steel 304L Bush Hex Pipe
- Stainless Steel 304L Round Pipe Supplier in Poland
- SS 304L ERW Pipes
- Stainless Steel 304L EFW Pipes in Qatar
- DIN 1.4306/1.4307 Steel Pipes
- Werkstoff Nr. 1.4306/1.4307 Steel Tubes
- X2CrNi18-9 / X2CrNi19-11 Pipes
- SUS 304L Pipes
- SUS 304L Rectangular Pipe
Countries We Export to
Nickel Super Alloys manufactures and exports Stainless Steel 304L Pipes to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia
Cities We Deliver to
Nickel Super Alloys manufactures and exports Stainless Steel 304L Pipes to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo