Alloy 20 Pipe & Tubes
ASTM B729 Alloy 20 Seamless Pipes, ASME SB 468 Alloy 20 Hydraulic Tubes, Alloy 20 Polished Pipes, Alloy 20 Capillary Tubes, Alloy 20 EFW Tubing, Alloy 20 Square Pipes Manufacturer in Mumbai, India.
Nickel Super Alloys is a Manufacturer & Supplier of alloy 20 pipes & alloy 20 tubes in india. These presented pipes & tubes are specifically developed and made-up making use of topnotch inputs to meet with the altering desires of our honored clients. These Alloy 20 pipes & tubes available in various forms like Seamless Pipes, ERW Pipes and Welded Pipes with or according to the customer need. Our product includes tubes and pipes, Alloy 20 Pipes, Alloy 20 Tubes, Alloy 20 Seamless Pipes & Tubes etc. Alloy 20 Welded Pipes is used for Control Valves, Pressure Relief Valves, and Centrifugal Pumps. Alloy 20 EFW Pipes is mainly constructed for Float level switches and Flow switches.
These Alloy 20 Seamless Pipes is a nickel – chromium – molybdenum stainless steel alloy that was developed for applications involving acid attack, specifically sulfuric acid. Specifically designed to withstand sulfuric acid, our Alloy 20 Welded Pipes offers excellent corrosion resistance. These Alloy 20 EFW Pipes has excellent resistance to corrosion, crevice corrosion, and pitting. Annealing of these Alloy 20 EFW Tubes should be between 1725 Degree F and 1850 Degree F for 30 minutes at temperature per inch of thickness. Our Alloy 20 ERW Tubes is also used for Heat exchangers and Bubble caps.
Alloy 20 Black Round Tubes, DIN 2.4660 Alloy 20 Round Pipes, ASME SB 729 Alloy 20 Capillary Tube, Alloy 20 ASTM B 464 Welded Tubes, Alloy 20 Rectangular Pipes, Alloy UNS N08020 ERW Pipes, Suppliers in India.
Key Charactristic:
- Corrosion resistance
- Resistance to oxidation and sulfidation
- Cryogenic strength
- Resistance to abrasion and erosion
- Surface finish
- Magnetic properties
- Ductility
- Elevated temperature strength
- Stability of properties in service
- Suitability for intended fabrication techniques
Alloy 20 Pipe & Tubes Specifications
| Grade | Alloy 20 (UNS N08020) |
| Size | 1/8"NB TO 30"NB IN |
| Standard | ASTM / ASME |
| Seamless Pipes Sizes | 1/8" NB to 48" |
| Welded Pipes Sizes | 1/8" NB to 48" |
| Form | Round, Square, Rectangular, Hydraulic Etc |
| Schedule | SCH20, SCH30, SCH40, STD, SCH80, XS, SCH60, SCH80, SCH120, SCH140, SCH160, XXS |
| Length | Single Random, Double Random & Cut Length. |
| Type | Seamless / ERW / Welded / Fabricated / EFW |
| End | Plain End, Beveled End, Treaded |
| Standard | Alloy 20 |
| Werkstoff Nr. | 2.4660 |
| UNS | N08020 |
| JIS | - |
| AFNOR | Z2NCUD31-20AZ |
| BS | - |
| GOST | - |
| EN | NiCr20CuMo |
Alloy 20 Pipe & Tubes Chemical Composition
| Alloy 20 | Ni | C | Mo | Mn | Si | Fe | Cu | S | P | Cr |
| 32 – 38 | 0.02 max | 2 – 3 | 1 – 2 | 0.7 max | Bal | 3 – 4 | 0.005 max | 0.02 max | 19 – 21 |
Alloy 20 Pipe & Tubes Mechanical Properties
| Density | Melting Point | Yield Strength (0.2%Offset) | Tensile Strength | Elongation |
| 8.1 g/cm3 | 1443 °C (2430 °F) | Psi – 35000 , MPa – 241 | Psi – 80000 , MPa – 551 | 30 % |
Other Types of Alloy 20 Pipe & Tubes
- Alloy 20 Seamless Pipes Supplier in UAE
- Alloy 20 Fabricated Pipes Manufacturer in India
- ASTM B 729 Welded Pipes
- Alloy 20 Seamless Tubing
- ASTM B 468 Alloy 20 Welded Tubes
- DIN 2.4660 Welded Tubing
- Alloy 20 Rectangular Pipe Distributors
- UNS N08020, DIN NR. 2.4660 Round Pipe
- WERKSTOFF NR. 2.4660 Welded Pipe
- Alloy N08020 Pipes
- Alloy 20 Pipes Exporter in Russia
- UNS N08020 Seamless Pipes
- Alloy 20 Welded Pipes Supplier in Poland
- Alloy 20 Hallow Pipe & Bush Pipes
- Alloy 20 Square Pipes in Qatar
- Alloy 20 ERW Pipes
- Alloy 20 EFW Pipes
- Alloy 20 Square Pipes
- UNS N08020 Hexagonal Pipe
- Alloy 20 Electric Resistance Welding Pipes
Countries We Export to
Nickel Super Alloys manufactures and exports Alloy 20 Pipes & Tubes to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia
Cities We Deliver to
Nickel Super Alloys manufactures and exports Alloy 20 Pipes & Tubes to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo