Cu-Ni 90-10 Pipes & Tubes
ASTM B466 Cupro Nickel 90/10 Seamless Pipes, Cu-Ni 90/10 Pipe, 90/10 Cupro Nickel Seamless Pipes & Tubes, Cupro Nickel WERKSTOFF NR. 2.0872 Pipe & Tubes Manufacturer in Mumbai,India.
Nickel Super Alloys is a renowned distributor of Copper Nickel 90 / 10 Pipes & Tubes, which is known for its moderate weldability, strength, and formability. Cupro Nickel 90 / 10 Seamless Pipes contain small but important additions of iron and manganese to enhance overall strength corrosion resistance. Cu-Ni 90 / 10 Welded Tubes offers excellent corrosion resistance, especially in marine salt water environments. Copper Nickel 90 / 10 EFW Pipes offers superior resistance to general corrosion and marine water attacks. Cupro Nickel 90 / 10 ERW Tubes have moderate strength and thermal stability in high temperature levels. Cu-Ni 90 / 10 RoundPipes havecopper (base metal with the largest individual content) and nickel with or without other elements.
Copper Nickel 90 / 10 Square Tubes is an alloy of copper that contains nickel and strengthening elements, such as iron and manganese. Cupro Nickel 90 / 10 Rectangular Pipes has additions of iron and manganese giving excellent corrosion resistance in fresh and sea water and anti-biofouling properties. Cu-Ni90 / 10 Electropolish Tubes were developed for and have been used extensively in seawater applications for over half a century. Copper Nickel 90 / 10 Hexagonal Pipes has impingement corrosion resulting from the turbulent flow of water containing air bubbles and silt flowing at a high velocity. Cupro Nickel 90 / 10 Heat Exchanger Tubes is the most commonly used wrought copper alloy for marine engineering.
90/10 Copper Nickel Pipes & Tubes, Cu-Ni 90/10 Hexagonal Pipe & Tubes, UNS C70600 Welded Pipe & Tubes, 90/10 Cu-Ni Seamless Pipes & Tubes, ASME SB466 Cupro Nickel Pipe & Tubes, Suppliers in India.
Key Charactristic:
- Corrosion resistance
- Resistance to oxidation and sulfidation
- Cryogenic strength
- Resistance to abrasion and erosion
- Surface finish
- Magnetic properties
- Ductility
- Elevated temperature strength
- Stability of properties in service
- Suitability for intended fabrication techniques
Cu-Ni 90-10 Pipes & Tubes Specifications
| Grade | Copper Nickel 90-10, UNS C70600 |
| Standard | ASTM B111, B151, B466 / ASME SB111, SB151, SB466, MIL-T-16420K, MIL-15005, CN102, C70610, CW352H, DEF STAN 02-879 Annex C, DEF STAN 02-779, NES 779, BS2870, BS2874, ASTM B151, EN 12163, NF A51-115, CuNi10Fe1Mn |
| Size | 1/4" NB To 12" NB |
| Out Diameter Size | 3mm OD to 114.3 mm OD |
| Form | Round, Square, Rectangular, Hydraulic Etc |
| Schedule | SCH20, SCH30, SCH40, STD, SCH80, XS, SCH60, SCH80, SCH120, SCH140, SCH160, XXS |
| Length | Single Random, Double Random & Cut Length. |
| Type | Seamless / ERW / Welded / Fabricated / EFW |
| End | Plain End, Beveled End, Treaded |
| Standard | Copper Nickel 90-10 |
| UNS | C70600 |
| WERKSTOFF NR. | 2.0872 |
Cu-Ni 90-10 Pipes & Tubes Chemical Composition
| Cu-Ni 90/10 | Cu | Pb | Mn | Fe | Zn | Ni |
| 88.6 min | 0.05 max | 1.0 max | 1.8 max | 1 max | 9-11 max |
Cu-Ni 90-10 Pipes & Tubes Mechanical Properties
| Density | Melting Point | Yield Strength (0.2%Offset) | Tensile Strength | Elongation |
| 8.1 g/cm3 | 1443 °C (2430 °F) | Psi – 35,000, MPa – 241 | Psi -80,000, MPa -551 | 30 % |
Other Types of Cu-Ni 90-10 Pipes & Tubes
- Cu-Ni 90-10 Pipes Supplier in UAE
- Cupro Nickel C70600 Seamless Pipes Manufacturer in India
- Cu-Ni 90-10 Welded Pipes
- 90-10 Cu-Ni Hallow Pipe
- Copper Nickel 90-10 Round Pipe
- Cu-Ni 90-10 Fabricated Pipes
- UNS C70600 Hexagonal Pipe Distributors
- Copper Nickel 90/10 Welded Tubing
- DIN 2.0872 Seamless Tubing
- ASTM B151 Hexagonal Pipe
- Copper Nickel 90/10 Seamless Pipes Exporter in Russia
- Copper Nickel 90/10 Seamless Tubing
- UNS C70600 Capillary Tubes Supplier in Poland
- Copper Nickel 90/10 ERW Tubes
- DIN 2.0872 Rectangular Seamless Pipes in Qatar
- Cu-Ni 90-10 Round Pipe
- ASTM B466 Cupro Nickel 90-10 Pipes
- Cu-Ni 90-10 ERW Pipes
- Cu-Ni C70600 Rectangular Pipe
- Cu-Ni 90-10 Pipes
Countries We Export to
Nickel Super Alloys manufactures and exports Cu-Ni 90-10 Pipes & Tubes to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia
Cities We Deliver to
Nickel Super Alloys manufactures and exports Cu-Ni 90-10 Pipes & Tubes to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo