Stainless Steel 310H Pipes & Tubes
ASTM A312 Stainless Steel Pipe, 310H Stainless Steel Seamless Pipes & Tubes, 310H SS Hexagonal Pipes & Tubes, Austenitic Stainless Steel 310H Pipes & Tubes, 310H SS Electropolished Pipes & Tubes Manufacturer in Mumbai,India.
Nickel Super Alloys is a prominent firm in manufacturing an exporting Stainless Steel 310H Pipes and Tubes, which displays excellent resistance to oxidation under mildly cyclic conditions. Stainless Steel 310H Seamless Pipes has good resistance to oxidation at temperatures of up to 1040 Degree C (1904 Degree F). Stainless Steel 310H Welded Tubes is ideally suited for high-temperature applications such as heat treatment and chemical processing equipment. Stainless Steel 310 HEFW Pipes is extensively inured to the effect of sulfurous gases, especially above 900 Degree C, is very low. Stainless Steel 310H ERW Tubes has high creep strength that resists oxidation at temperatures up to 2000 Degree F in dry air.
A specific feature for Stainless Steel 310H Round Pipes is high chromium and high nickel contents. The high nickel and chromium contents of Stainless Steel 310H Square Tubesimpart excellent elevated temperature strength and resistance to oxidation. The high chromium and nickel contents of Stainless Steel 310H Rectangular Pipes also provide comparable corrosion resistance. Stainless Steel 310H Electropolish Tubes resists oxidation up to 2010 Degree F (1100 Degree C) under mildly cyclic conditions. Stainless Steel 310H Hexagonal Pipes is used at temperatures up to 1150 Degree C in continuous service, and 1035 Degree C in intermittent service. Stainless Steel UNS S31009 Tubes is typically used for elevated temperature applications as its high chromium and nickel content provide solid corrosion resistance.
ASTM A312 TP 310H Stainless Steel Seamless Pipes & Tubes, SS UNS S31009 Welded Pipe, Stainless Steel 310H Hallow Pipes & Tubes, SS TP310H Seamless Pipe & Tubes, SS 310H Bush Hex Pipe, Suppliers in India.
Key Charactristic:
- Corrosion resistance
- Resistance to oxidation and sulfidation
- Cryogenic strength
- Resistance to abrasion and erosion
- Surface finish
- Magnetic properties
- Ductility
- Elevated temperature strength
- Stability of properties in service
- Suitability for intended fabrication techniques
SS 310H Pipe Stock Size Range and Specifications
| Grade | Stainless Steel 310H / SS TP 310H |
| Size | 1/2" NB TO 24" |
| Standard | ASTM A/ ASME SA213 / A249 / A269/ A312 / A358 CL. I to V ASTM A789 / A790 |
| Steel 310H Pipes | 1/2" NB TO 24" |
| Form | Round, Square, Rectangular, Hydraulic Etc |
| Schedule | SCH20, SCH30, SCH40, STD, SCH80, XS, SCH60, SCH80, SCH120, SCH140, SCH160, XXS |
| Length | Single Random, Double Random & Cut Length. |
| Type | Seamless / ERW / Welded / Fabricated / EFW |
| End | Plain End, Beveled End, Treaded |
| Standard | SS 310H |
| Werkstoff Nr. | - |
| UNS | S31009 |
| JIS | - |
| AFNOR | - |
| BS | - |
| GOST | - |
| EN | - |
310H Stainless Steel Pipes Chemical Composition
| Grade | C | Mn | Si | P | S | Cr | Mo | Ni | N | |
| 310H | min. | 0.04 | – | – | – | – | 24.0 | – | 19.0 | – |
| max. | 0.10 | 2.0 | 1.00 | 0.045 | 0.03 | 26.0 | 21.0 | – | ||
Stainless Steel 310H Pipe Mechanical Properties
| Grade | Tensile Strength (MPa) min | Yield Strength 0.2% Proof (MPa) min | Elongation (% in 50mm) min | Hardness | |
| Rockwell B (HR B) max | Brinell (HB) max | ||||
| 310H | 515 | 205 | 40 | 95 | 217 |
Other Types of Stainless Steel 310H Pipes & Stainless Steel Tubes
- SS 310H Seamless Pipes Supplier in UAE
- Stainless Steel 310H Pipes Manufacturer in India
- SS 310H Welded Pipes
- ASTM A312 TP 310H Fabricated Pipes
- Stainless Steel 310H Tubes
- SS 310H Round Tubes
- Stainless Steel 310H Square Pipe
- 310H Electropolish ERW Pipes
- UNS S31009 Hexagonal Pipe
- 310H Stainless Stel Hallow Pipe
- UNS S31009 Welded Tubes Exporter in Russia
- Steel 310H Bush Hex Pipe
- Stainless Steel 310H Round Pipe Supplier in Poland
- SS 310H ERW Pipes
- Stainless Steel 310H EFW Pipes in Qatar
- Stainless Steel 310H Steel Pipes
- Stainless Steel 310H Tubing
- Stainless Steel 310H Tubes
- SUS 310H Pipes
- SUS 310H Rectangular Pipe
Countries We Export to
Nickel Super Alloys manufactures and exports Stainless Steel 310H Pipes to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia
Cities We Deliver to
Nickel Super Alloys manufactures and exports Stainless Steel 310H Pipes to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo