Stainless Steel 316L Pipes & Tubes
ASTM A249 TP 316L SS Seamless Pipes & Tubes, ASTM A213 SS TP 316L Seamless Tubing, 316L SS Polished Pipes, ASTM A213 SS 316L Pipes, TP 316L SS ERW Pipes, Manufacturer in Mumbai,India.
Nickel Super Alloys is one of the leading distributor and supplier of Stainless Steel 316L Pipes and Tubes, which is resistant to certain types of interactions. Stainless Steel 316L Seamless Pipes possesses excellent mechanical properties. Stainless Steel 316L Welded Tubes has particularly higher resistance to pitting and crevice corrosion in chloride environments. Stainless Steel 316L EFW Pipes can withstand much more time and abuse before showing signs of wear. Additions of molybdenum in Stainless Steel 316L ERW Tubes increase corrosion resistance in reducing acids and against pitting attack in chloride solutions. The addition of molybdenum and slightly higher nickel content make Stainless Steel 316L Round Pipes suitable for architectural applications.
The resultant composition of Stainless Steel 316L Square Tubes gives much increased corrosion resistance in many aggressive environments. Stainless Steel 316L Rectangular Pipes has good elevated temperature strength. These Stainless Steel 316L Electropolish Tubes are more resistant to general corrosion and pitting/crevices than conventional austenitic stainless steels. Stainless Steel 316L Hexagonal Pipes is commonly used in chemical and petrochemical industry. Stainless Steel 316L Bush Hex Tubes is immune from sensitization (grain boundary carbide precipitation). Stainless Steel UNS S31603 Pipes has higher creep resistance. Stainless Steel WNR 1.4404 Tubes is developed to provide improved corrosion resistance in moderately corrosive environments. The low carbon chemistry of 316LS tainless Steel Pipes combined with an addition of nitrogen enables to meet excellent mechanical properties.
A312 Stainless Steel TP316L Round Pipes & Tubes, 316L Stainless Steel EFW Tubing, Stainless Steel TP316L Black Round Tubes, Stainless Steel 316L Welded Tubes, SS UNS S31603 Square Pipes Suppliers in India.
Key Charactristic:
- Corrosion resistance
- Resistance to oxidation and sulfidation
- Cryogenic strength
- Resistance to abrasion and erosion
- Surface finish
- Magnetic properties
- Ductility
- Elevated temperature strength
- Stability of properties in service
- Suitability for intended fabrication techniques
SS 316L Pipe Stock Size Range and Specifications
| Grade | SS 316 / TP 316 Stainless Steel Pipes / Stainless Steel 316L / TP 316L Stainless Steel Pipes |
| Size | 1/2" NB - 24" NB |
| Standard | ASTM A/ ASME / SA213 / A249 / A269 / A312 / A358 CL. I to V |
| Form | Round Pipes, Square Pipes, Rectangular Pipe, “U” Shape, Oval Pipes, Hydraulic Pipes |
| Schedule | SCH 5, SCH10, SCH 40, SCH 80, SCH 80S, SCH 160, SCH XXS, SCH XS, XXS |
| Length | Single Random, Double Random & Cut Length. |
| Type | Seamless / ERW / Welded / Fabricated / EFW /LSAW |
| End | Plain End, Beveled End, Treaded |
| Standard | SS 316 | SS 316L |
| UNS | S31600 | S31603 |
| WERKSTOFF NR. | 1.4401 / 1.4436 | 1.4404 / 1.4435 |
| AFNOR | Z7CND17‐11‐02 | Z3CND17‐11‐02 / Z3CND18‐14‐03 |
| JIS | SUS 316 | SUS 316L |
| GOST | - | 03Ch17N14M3 / 03Ch17N14M2 |
| BS | 316S31 / 316S33 | 316S11 / 316S13 |
| EN | X5CrNiMo17-12-2 / X3CrNiMo17-13-3 | X2CrNiMo17-12-2 / X2CrNiMo18-14-3 |
316L Stainless Steel Pipes Chemical Composition
| Grade | C | Mn | Si | P | S | Cr | Mo | Ni | N | |
| 316 – 316L | min. | – | – | – | – | – | 16.0 | 2.0 | 10.0 | – |
| max. | 0.08 | 2.0 | 0.75 | 0.045 | 0.03 | 18.0 | 3.0 | 14.0 | 0.10 | |
Stainless Steel 316L Pipe Mechanical Properties
| Grade | Tensile Strength (MPa) min | Yield Strength 0.2% Proof (MPa) min | Elongation (% in 50mm) min | Hardness | |
| Rockwell B (HR B) max | Brinell (HB) max | ||||
| 316 – 316L | 515 | 205 | 40 | 95 | 217 |
Other Types of Stainless Steel 316L Pipes & Stainless Steel Tubes
- SS 316L Seamless Pipes Supplier in UAE
- Stainless Steel 316L Pipes Manufacturer in India
- SS 316L Welded Pipes
- ASTM A312 TP 316L Fabricated Pipes
- Stainless Steel 316L Tubes
- SS 316L Round Tubes
- Stainless Steel 316L Square Pipe
- 316L Electropolish ERW Pipes
- UNS S31603 Hexagonal Pipe
- 316L Stainless Stel Hallow Pipe
- UNS S31603 Welded Tubes Exporter in Russia
- Steel 316L Bush Hex Pipe
- Stainless Steel 316L Round Pipe Supplier in Poland
- SS 316L ERW Pipes
- Stainless Steel 316L EFW Pipes in Qatar
- DIN 1.4401 / 1.4436 Steel Pipes
- Werkstoff Nr. 1.4404 / 1.4435 Steel Tubes
- X2CrNiMo17-12-2 / X2CrNiMo18-14-3 Pipes
- SUS 316L Pipes
- SUS 316L Rectangular Pipe
Countries We Export to
Nickel Super Alloys manufactures and exports Stainless Steel 316L Pipes to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia
Cities We Deliver to
Nickel Super Alloys manufactures and exports Stainless Steel 316L Pipes to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo