Monel 400 Pipes & Tubes
Monel Alloy 400 EFW Tubing, DIN 2.4360 Hydraulic Tubes, JIS NW 4400 Seamless Pipes, Monel 400 Welded Tubes, Monel Alloy 400 Square Pipes, ASME SB 165 Monel 400 Black Round Tubes Manufacturer in Mumbai,India.
Nickel Super Alloys is one of the known suppliers of Monel Alloy 400 Pipes & Tubes, which exhibits good corrosion resistance.Monel 400 Seamless Pipes is resistant to sea water and steam at high temperatures as well as to salt and caustic solutions. Monel 400 Welded Pipes is a solid-solution alloy that can be hardened only by cold working. Monel 400 EFW Pipes is a nickel-copper alloy that is resistant to corrosion in many environments.Monel 400 ERWPipesis a nickel-copper alloy with excellent corrosion resistance in a wide variety of media. Stronger than pure nickel, Monel 400 Round Pipes is resistant to corrosion by many agents, including rapidly flowing seawater.
Monel 400 Square Pipes is a single phase and solid-solution nickel-copper alloy. Monel 400 Rectangular Pipes has high strength and toughness over a wide temperature range and is resistant to many corrosive environments. Monel 400 Electropolish Pipes is widely used in the chemical, oil and marine industries. Monel 400 Hexagonal Pipes has low corrosion rate in flowing seawater, therefore it is widely used in marine applications. Monel 400 Hallow Pipes is characterized by moderate strength, good general corrosion resistance, good weldability, and good toughness. Monel 400 Bush Hex Pipes has superb corrosion resistance, particularly in neutral and alkaline salts. Monel UNS N04400 Pipes is well known for its elevatedpotency and corrosion resistant properties.
Monel 400 Rectangular Pipes, ASTM B 163 Round Pipes, UNS N04400 Capillary Tubes, Monel JIS NW 4400 Welded Tubing, Monel 400 Polished Pipes, Monel UNS N04400 ERW Pipes, Alloy 400 Capillary Tubes, Suppliers in India.
Key Charactristic:
- Corrosion resistance
- Resistance to oxidation and sulfidation
- Cryogenic strength
- Resistance to abrasion and erosion
- Surface finish
- Magnetic properties
- Ductility
- Elevated temperature strength
- Stability of properties in service
- Suitability for intended fabrication techniques
Monel 400 Pipe & Tubes Specifications
| Grade | Monel 400 (UNS No. N04400) |
| Size | 15"NB TO 150"NB IN |
| Standard | ASTM A163, ASME SB163 |
| Range | 6.35 mm OD upto 254 mm OD in 0.6 TO 20 mm thickness. |
| Form | Round, Square, Rectangular, Hydraulic Etc |
| Schedule | SCH20, SCH30, SCH40, STD, SCH80, XS, SCH60, SCH80, SCH120, SCH140, SCH160, XXS |
| Length | Single Random, Double Random & Cut Length. |
| Type | Seamless / ERW / Welded / Fabricated / EFW |
| End | Plain End, Beveled End, Treaded |
| Standard | Monel 400 |
| Werkstoff Nr. | 2.4360 |
| UNS | N04400 |
| JIS | NW 4400 |
| AFNOR | NU-30M |
| BS | NA 13 |
| GOST | МНЖМц 28-2,5-1,5 |
| EN | NiCu30Fe |
Monel 400 Pipe & Tubes Chemical Composition
| Monel 400 | Ni | C | Al | Mn | Si | Fe | Cu | S | Co | Cr |
| 63.0 min | 0.3 max | 0.50 max | 2.0 max | 0.5 max | 1.0 – 2.5 | 28.0 – 34.0 | 0.02 max | – | – |
Monel 400 Pipe & Tubes Mechanical Properties
| Density | Melting Point | Yield Strength (0.2%Offset) | Tensile Strength | Elongation |
| 8.8 g/cm3 | 1350 °C (2460 °F) | Psi – 35,000 , MPa – 240 | Psi – 80,000 , MPa – 550 | 40 % |
Other Types of Monel 400 Pipe & Tubes
- Monel 400 Seamless Pipes Supplier in UAE
- Monel 400 Pipes Manufacturer in India
- Monel 400 Welded Pipes
- Monel 400 Rectangular Pipe
- Monel 400 Fabricated Pipes
- Monel 400 Round Pipe
- Monel 400 Square Pipe Distributors
- UNS N04400 Hexagonal Pipe
- Monel 400 Hallow Pipe
- DIN 2.4360 Rectangular Seamless Pipes
- ASME SB 163 Monel 400 ERW Pipes Exporter in Russia
- ASTM B 163 Alloy 400 Welded Pipes
- JIS NW 4400 Welded Tubing Supplier in Poland
- Monel Alloy 400 Seamless Tubing
- ASME SB 165 Monel 400 Welded Tubes in Qatar
- UNS N04400 Capillary Tubes
- Monel 400 ERW Tubes
- UNS N04400 Monel Coiled Seamless Tubing
- 400 Monel Alloy Round Tubing
- DIN 2.4360 Rectangular Seamless Pipes
Countries We Export to
Nickel Super Alloys manufactures and exports Monel 400 Pipes & Tubes to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia
Cities We Deliver to
Nickel Super Alloys manufactures and exports Monel 400 Pipes & Tubes to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo