Stainless Steel 904L Pipe Fittings
Stainless Steel UNS N08904 Seamless Pipe Fittings, SS 904L Pipe Fittings, 904L Stainless Steel End Cap, SS 904L Short Radius Elbow, ASTM B366 904L Stainless Steel 90 degree Elbow Manufacturer in Mumbai,India.
Nickel Super Alloys is one of known manufacturing and stockist firm of Stainless Steel 904L Butt Weld Pipe Fittings, which has greater amounts of chromium and nickel. Stainless Steel 904L Elbow Pipe Fittings is also highly resistant to chloride attack – both pitting and crevice corrosion and SCC. Stainless Steel 904L Tee Pipe Fittings has greater resistance reducing acids. The low carbon content of Stainless Steel 904L Cross Pipe Fittings improves cleanliness and weld strength. The addition of copper to Stainless Steel 904L Reducer Pipe Fittings gives it corrosion resistant properties superior to the conventional chrome nickel alloy. Stainless Steel 904L Bend Pipe Fittings stands up extremely well to chlorides in the environment for low pitting and crevice corrosion, as well as stress corrosion cracking.
Stainless Steel 904L Stub End Pipe Fittings is used extensively in the chemical process industry including the production of phosphate-based fertilizers. Stainless Steel 904L End Cap Pipe Fittings is used in bleaching tanks for the paper industry. Stainless Steel 904L Dish Cap Pipe Fittings is added with copper to improve its resistance to strong reducing acids, such as sulfuric acid. Stainless Steel UNS N08904 Pipe Fittings is a low carbon version of steel which offers other benefits to users including non-magnetic. Stainless Steel DIN 1.4539 Pipe Fittings prevents attack by sulfuric, acetic and phosphoric acids. 904L Stainless Steel Butt Weld Fittings provides good chloride stress corrosion cracking resistance, pitting and general corrosion resistance superior to molybdenum enhanced stainless steels.
ASTM B366 904L Stainless Steel 90 degree Elbow, SS 904L Equal Tee, ANSI B16.9 Stainless Steel 904L Welded Buttweld Fittings, ASME SB366 SS 904L Long Stub, Stainless Steel 1.5d Pipe Bend Suppliers in India.
Key Charactristic:
- Corrosion resistance
- Resistance to oxidation and sulfidation
- Cryogenic strength
- Resistance to abrasion and erosion
- Surface finish
- Magnetic properties
- Ductility
- Elevated temperature strength
- Stability of properties in service
- Suitability for intended fabrication techniques
Stainless Steel 904L Pipe Fittings Specifications
| Grade | SS 904L | UNS N08904 |
| Standard | ASTM B366 / ASME SB366 |
| Dimensions | ANSI/ASME B16.9, B16.28, MSS-SP-43. |
| Thickness | 5s, 10s, 40s, 80s, 10, 20, 40, STD, 60, 80, XS, 100, 120, 140, 160, XXS available with NACE MR 01-75 |
| Size | 1/2" NB - 48" NB |
| Form | 90 Elbow, 45 Elbow, Long Radius Elbow, Short Radius Elbow, Concentric Reducer, Eccentric Reducer, Equal Tee, Unequal Tee, Lateral Tee, Cross, Bends 1.5d, 3d, 5d, 10d, U bend, 180 Deg Bend, Short Stub End, Long stub end, End Cap, Dish Cap |
| Schedule | SCH 5 To SCH XXS |
| Type | Seamless / Welded / Fabricated |
| Grade | UNS No | Old British | Euronorm | Swedish SS | Japanese JIS | ||
| BS | En | No | Name | ||||
| 904L | N08904 | 904S13 | X1NiCrMoCu25-20-5 | 1.4539 | – | – | SUS 904L |
Stainless Steel 904L Pipe Fittings Chemical Composition
| Grade | C | Mn | Si | P | S | Cr | Mo | Ni | N | |
| 904L | min. | – | – | – | – | – | 19.0 | 4.00 | 23.00 | 0.10 |
| max. | 0.20 | 2.00 | 1.00 | 0.045 | 0.035 | 23.0 | 5.00 | 28.00 | 0.25 | |
Stainless Steel 904L Pipe Fittings Mechanical Properties
| Grade | Tensile Strength (MPa) min | Yield Strength 0.2% Proof (MPa) min | Elongation (% in 50mm) min | Hardness | |
| Rockwell B (HR B) max | Brinell (HB) max | ||||
| 904L | 490 | 220 | 35 | 70-90 typical | – |
Other Types of Stainless Steel 904L Pipe Fittings
- SS 904L Buttweld Tee Supplier in UAE
- Stainless UNS N08904 Cross Manufacturer in India
- SS 904L Butwteld Tee
- DIN 1.4539 45deg.Elbow
- DIN 1.4539 Buttweld Pipe Fittings
- 904L Steel Short Radius Elbow
- UNS N08904 Ecentric Reducer Distributors
- SS 904L Buttweld Pipe Fitting
- ASME B16.28 Stub End
- SS 904L Concentric Reducer
- ASME SA403 SS Long Radius Elbow Exporter in Russia
- Stainless Steel 904L U Bend
- WNR. 1.4539 SS 347H Stub End Supplier in Poland
- 904L Short Radius Elbow
- WP 904L Steel Equal Tee in Qatar
- UNS N08904 End Cap
- ASME SA403 Concentric Reducer
- SS N08904 Seamless Fitting
- Stainless Steel 904L 45 Elbow
- SS 904L Pipe Bends
Countries We Export to
Nickel Super Alloys manufactures and exports Stainless Steel 904L Pipe Fittings to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia
Cities We Deliver to
Nickel Super Alloys manufactures and exports Stainless Steel 904L Pipe Fittings to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo