Alloy 20 Pipe Fittings
Alloy 20 Pipe Fittings, Alloy WERKSTOFF NR. 2.4660 Cross, Alloy 20 Pipe Elbow, Alloy 20 Pipe Bend, ANSI B16.9 Alloy 20 Eccentric & Concentirc Reducer, Alloy 20 90 Degree Elbow Manufacturer in Mumbai, India.
Nickel Super Alloys is one of the known manufacturers and exporters of Alloy 20 Butt Weld Pipe Fittings, which is designed specifically to withstand sulfuric acid. Alloy 20 Elbow Pipe Fittingsis an austenitic stainless steel developed for applications involving sulfuric acid. Alloy 20 Tee Pipe Fittingsis developed for maximum resistance to acid attack, specifically sulfuric acid. With additions of Copper and Molybdenum, Alloy 20 Cross Pipe Fittings provides resistance to hostile environments, pitting, and crevice corrosion. Alloy 20 Pipe Reducer Fittingshas excellent corrosion resistance to a number of different media and proves to be useful in a number of applications. Alloy 20 Bend Pipe Fittingshas a very tight chemistry range within the broad limits to optimize the alloy’s performance.
Alloy 20 Stub End Pipe Fittings also has good mechanical properties at both ambient and elevated temperatures.For stabilization against sensitization and resultant inter-granular corrosion, Alloy 20 End Cap Pipe Fittings contains niobium.A nickel-iron-chromium grade, Alloy 20 Dish Cap Pipe Fittingsis ideal for a wide range of corrosive environments. Alloy 20 Lateral Tee Pipe Fittingscombines excellent corrosion resistance with elevated mechanical properties and relatively easy fabrication. Alloy 20 Concentric Reducer Pipe Fittings is well suited to the productiono fexplosives, gasoline, solvents, inorganic and organic chemicals. Alloy 20 Eccentric Reducer Pipe Fittingsis a super-austenitic stainless alloy developed for maximum corrosion resistance to sulfuric acid.
Alloy UNS N08020 Seamless Pipe Fittings, Carpenter 20 Equal & Unequal Tee, Alloy 20 Long & Short Radius Elbow, ASME SB366 Alloy 20 Long Stub End, Alloy 20 180 Deg bend, Alloy 20 Cross Suppliers in India.
Key Charactristic:
- Corrosion resistance
- Resistance to oxidation and sulfidation
- Cryogenic strength
- Resistance to abrasion and erosion
- Surface finish
- Magnetic properties
- Ductility
- Elevated temperature strength
- Stability of properties in service
- Suitability for intended fabrication techniques
Alloy 20 Pipe Fittings Specifications
| Grade | Alloy 20 | UNS N08020 |
| Standard | ASTM B366 / ASME SB366 |
| Dimensions | ANSI/ASME B16.9, B16.28, MSS-SP-43. |
| Thickness | 5s, 10s, 40s, 80s, 10, 20, 40, STD, 60, 80, XS, 100, 120, 140, 160, XXS available with NACE MR 01-75 |
| Size | 1/2" NB - 24" NB |
| Form | 90 Elbow, 45 Elbow, Long Radius Elbow, Short Radius Elbow, Concentric Reducer, Eccentric Reducer, Equal Tee, Unequal Tee, Lateral Tee, Cross, Bends 1.5d, 3d, 5d, 10d, U bend, 180 Deg Bend, Short Stub End, Long stub end, End Cap, Dish Cap |
| Schedule | SCH 5 To SCH XXS |
| Type | Seamless / Welded / Fabricated |
| Standard | Alloy 20 |
| Werkstoff Nr. | 2.4660 |
| UNS | N08020 |
| JIS | - |
| AFNOR | Z2NCUD31-20AZ |
| SIS | - |
| GOST | - |
| EN | NiCr20CuMo |
Alloy 20 Pipe Fittings Chemical Composition
| Alloy 20 | Ni | C | Mo | Mn | Si | Fe | Cu | S | P | Cr |
| 32 – 38 | 0.02 max | 2 – 3 | 1 – 2 | 0.7 max | Bal | 3 – 4 | 0.005 max | 0.02 max | 19 – 21 |
Alloy 20 Pipe Fittings Mechanical Properties
| Density | Melting Point | Yield Strength (0.2%Offset) | Tensile Strength | Elongation |
| 8.1 g/cm3 | 1443 °C (2430 °F) | Psi – 35000 , MPa – 241 | Psi – 80000 , MPa – 551 | 30 % |
Other Types of Alloy 20 Pipe Fittings
- Alloy 20 Buttweld Tee Supplier in UAE
- UNS N08020 Cross Manufacturer in India
- DIN 2.4660 Butwteld Tee
- DIN 2.4660 45 deg.Elbow
- Alloy 20 Buttweld Pipe Fittings
- Alloy 20 Short Radius Elbow
- UNS N08020 Ecentric Reducer Distributors
- Alloy 20 Buttweld Pipe Fitting
- ASME SB366 Stub End
- Alloy 20 Concentric Reducer
- Alloy 20 Long Radius Elbow Exporter in Russia
- Alloy 20 U Bend
- Alloy 20 Stub End Supplier in Poland
- Alloy 20 Short Radius Elbow
- Alloy 20 Equal Tee in Qatar
- UNS N08020 End Cap
- ASME SB366 Concentric Reducer
- Alloy 20 Seamless Fitting
- Alloy 20 180 Deg Elbow
- Alloy 20 Pipe Bends
Countries We Export to
Nickel Super Alloys manufactures and exports Alloy 20 Pipe Fittings to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia
Cities We Deliver to
Nickel Super Alloys manufactures and exports Alloy 20 Pipe Fittings to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo