Monel 400 Pipe Fittings
Monel 400 Pipe Fittings, ASTM B366 Monel 400 Pipe Elbow, Alloy ANSI B16.9 Short & Long Radius Elbow, Monel 400 10d Pipe Bend, UNS N04400 Seamless Pipe Fittings, WERKSTOFF NR. 2.4360 Cross Manufacturer in Mumbai, India.
Nickel Super Alloys is one of the known suppliers of Monel Alloy 400 Butt Weld Pipe Fittings, which works in a wide range of temperatures. Monel 400 Elbow Pipe Fittingsis also one of a limited number of alloys that can be used in conjunction with hydrofluoric acid and fluorine. Monel 400 Tee Pipe Fittings is useful at temperatures up to 1000 Degree F (538 Degree C). Monel 400 Reducer Pipe Fittingsis a solid solution alloy that can only be hardened by cold working. Monel 400 Cross Pipe Fittingshas high strength and toughness over a wide temperature range. Monel 400 Cap Pipe Fittings consists of two crystalline solids that, together, form a single new solid. Monel 400 Eccentric Reducer Pipe Fittings is characterized by good general corrosion resistance.
Monel 400 Bend Pipe Fittings can be fabricated readily by hot- and cold-working, welding and machining. Monel 400 Stub End Pipe Fittings offers superior resistance to several corrosive environments over temperatures ranging from sub-zero to 800 Degree F. The machinability of Monel 400 End Cap Pipe Fittings is difficult as it work-hardens during machining. Monel 400 Dish Cap Pipe Fittings is used in many fields, especially marine and chemical processing. As a solution strengthened material, Monel 400 Lateral Tee Pipe Fittings displays good toughness, strength, and corrosion resistance at temperatures up to 400 Degree C. Monel 400 Concentric Reducer Pipe Fittings has excellent resistance to stress corrosion cracking in most fresh waters.
Monel 400 5D Pipe Bend, ASME SB366 Monel 400 Long Stub, ANSI B16.9 400 Monel Reducer, Alloy 400 Equal Tee, DIN 2.4360 600 Pipe bend, Monel 400 Equal Tee, UNS N04400 Reducing Tee, 400 Monel Unequal Cross Suppliers in India.
Key Charactristic:
- Corrosion resistance
- Resistance to oxidation and sulfidation
- Cryogenic strength
- Resistance to abrasion and erosion
- Surface finish
- Magnetic properties
- Ductility
- Elevated temperature strength
- Stability of properties in service
- Suitability for intended fabrication techniques
Monel 400 Pipe Fittings Specifications
| Grade | Monel 400 / UNS N04400 |
| Standard | ASTM B366, ASME SB366 |
| Dimensions | ASME B16.28, ASME/ANSI B16.9, MSS-SP-43 |
| Monel 400 Seamless Fittings | 1/2" NB - 10" NB |
| Monel 400 Welded Fittings | 1/2" NB - 48" NB |
| Form | 90 Elbow, 45 Elbow, Long Radius Elbow, Short Radius Elbow, Concentric Reducer, Eccentric Reducer, Equal Tee, Unequal Tee, Lateral Tee, Cross, Bends 1.5d, 3d, 5d, 10d, U bend, 180 Deg Bend, Short Stub End, Long stub end, End Cap, Dish Cap |
| Schedule | SCH 5 To SCH XXS |
| Wall Thickness | from 2 to 40 mm |
| Type | Seamless / Welded / Fabricated |
| Standard | Monel 400 |
| Werkstoff Nr. | 2.4360 |
| UNS | N04400 |
| JIS | NW 4400 |
| AFNOR | NU-30M |
| BS | NA 13 |
| GOST | МНЖМц 28-2,5-1,5 |
| EN | NiCu30Fe |
Monel 400 Pipe Fittings Chemical Composition
| Monel 400 | Ni | C | Al | Mn | Si | Fe | Cu | S | Co | Cr |
| 63.0 min | 0.3 max | 0.50 max | 2.0 max | 0.5 max | 1.0 – 2.5 | 28.0 – 34.0 | 0.02 max | – | – |
Monel 400 Pipe Fittings Mechanical Properties
| Density | Melting Point | Yield Strength (0.2%Offset) | Tensile Strength | Elongation |
| 8.8 g/cm3 | 1350 °C (2460 °F) | Psi – 35,000 , MPa – 240 | Psi – 80,000 , MPa – 550 | 40 % |
Other Types of Monel 400 Pipe Fittings
- Monel 400 Buttweld Tee Supplier in UAE
- UNS N04400 Cross Manufacturer in India
- DIN 2.4360 Butwteld Tee
- DIN 2.4360 45 deg.Elbow
- Monel 400 Buttweld Pipe Fittings
- Monel 400 Short Radius Elbow
- UNS N04400 Ecentric Reducer Distributors
- Monel 400 Buttweld Pipe Fitting
- ASME SB366 Stub End
- 400 Monel Concentric Reducer
- Monel 400 Long Radius Elbow Exporter in Russia
- Monel 400 U Bend
- Monel 400 Stub End Supplier in Poland
- 400 Monel Short Radius Elbow
- Monel 400 Equal Tee in Qatar
- UNS N04400 End Cap
- ASME SB366 Concentric Reducer
- Monel 400 Seamless Fitting
- Monel 400 180 Deg Elbow
- Monel 400 Pipe Bends
Countries We Export to
Nickel Super Alloys manufactures and exports Monel 400 Pipe Fittings to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia
Cities We Deliver to
Nickel Super Alloys manufactures and exports Monel 400 Pipe Fittings to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo