Stainless Steel 446 Pipe Fittings
ASME SA403 SS 446 Long Stub, Stainless Steel 3D Pipe Bend, ANSI B16.9 SS 446 Concentric Reducer, Stainless Steel 446 Lateral Pipe Tee, SS 446 Equal Tee SS 446 Stub End Manufacturer in Mumbai,India.
Nickel Super Alloys is a popular firm that exports and manufactures these Stainless Steel 446 Butt Weld Pipe Fittings, which possesses good mechanical properties. Stainless Steel 446 Elbow Pipe Fittings combines high strength with the corrosion resistance of alloy. Fracture toughness and hardness of Stainless Steel 446 Tee Pipe Fittings exceeds those of other bearing steels. Further, Stainless Steel 446 Cross Pipe Fittings has excellent sulfurizing atmospheres abrasion. Stainless Steel 446 Reducer Pipe Fittings is the most oxidation resistant steel among the 400 series stainless. In addition, Stainless Steel 446 Bend Pipe Fittings is used in boiler baffles, X-ray tube bases and furnace parts.
Stainless Steel 446 Stub End Pipe Fittings provides good resistance to high temperature oxidation and corrosion. Stainless Steel 446 End Cap Pipe Fittings is most commonly used between the ranges of 1500 Degree F – 2100 Degree F. Stainless Steel 446 Dish Cap Pipe Fittings is often used for glass molds and stationary soot blowers in steam boilers. 446 Stainless Steel Pipe Fittings is extensively inured to the effects of sulfurous gases. Stainless Steel UNS S44600 Pipe Fittings has very good resistance to oxidation in air. Stainless Steel DIN 1.4762 Pipe Fittings has typical annealing temperatures with 730 Degree C – 815 Degree C; followed by air or water quench. Stainless Steel 446 Lateral Tee Pipe Fittings is very weldable, where hardening is accomplished by a short – time and simple low – temperature treatment.
SS 446 Buttweld Pipe Bend, Stainless Steel 446 End Cap, SS 446 Pipe Elbow, 446 Stainless Steel Short Stub end, SS 446 Pipe End & Dish Cap, SS 347 Cross, SS 410 5d Pipe Bend, ASME SA403 SS 446 Short Stub Suppliers in India.
Key Charactristic:
- Corrosion resistance
- Resistance to oxidation and sulfidation
- Cryogenic strength
- Resistance to abrasion and erosion
- Surface finish
- Magnetic properties
- Ductility
- Elevated temperature strength
- Stability of properties in service
- Suitability for intended fabrication techniques
Stainless Steel 446 Pipe Fittings Specifications
| Grade | SS 446 | UNS S44600 |
| Standard | ASTM A403 / ASME SA403 |
| Dimensions | ANSI/ASME B16.9, B16.28, MSS-SP-43. |
| Thickness | 5s, 10s, 40s, 80s, 10, 20, 40, STD, 60, 80, XS, 100, 120, 140, 160, XXS available with NACE MR 01-75 |
| Size | 1/2" NB - 48" NB |
| Form | 90 Elbow, 45 Elbow, Long Radius Elbow, Short Radius Elbow, Concentric Reducer, Eccentric Reducer, Equal Tee, Unequal Tee, Lateral Tee, Cross, Bends 1.5d, 3d, 5d, 10d, U bend, 180 Deg Bend, Short Stub End, Long stub end, End Cap, Dish Cap |
| Schedule | SCH 5 To SCH XXS |
| Type | Seamless / Welded / Fabricated |
| Grade | UNS No | Old British | Euronorm | Swedish SS | Japanese JIS | ||
| BS | En | No | Name | ||||
| 446 | S44600 | – | – | 1.4762 / 1.4763 | – | – | – |
Stainless Steel 446 Pipe Fittings Chemical Composition
| Grade | C | Mn | Si | P | S | Cr | Mo | Ni | N | |
| 446 | min. | – | – | – | – | – | 23.0 | – | – | 0.10 |
| max. | 0.2 | 1.5 | 0.75 | 0.040 | 0.030 | 30.0 | – | 0.50 | 0.25 | |
Stainless Steel 446 Pipe Fittings Mechanical Properties
| Grade | Tensile Strength (MPa) min | Yield Strength 0.2% Proof (MPa) min | Elongation (% in 50mm) min | Hardness | |
| Rockwell B (HR B) max | Brinell (HB) max | ||||
| 446 | 485 | 275 | 20 | 92 | 201 |
Other Types of Stainless Steel 446 Pipe Fittings
- SS 446 Buttweld Tee Supplier in UAE
- Stainless UNS S44600 Cross Manufacturer in India
- SS 446 Butwteld Tee
- DIN 1.4762 45deg.Elbow
- DIN 1.4763 Buttweld Pipe Fittings
- 446 Steel Short Radius Elbow
- UNS S44600 Ecentric Reducer Distributors
- SS 446 Buttweld Pipe Fitting
- ASME B16.28 Stub End
- SS 446 Concentric Reducer
- ASME SA403 SS Long Radius Elbow Exporter in Russia
- Stainless Steel 446 U Bend
- WNR. 1.4762 / 1.4763 SS 347H Stub End Supplier in Poland
- 446 Short Radius Elbow
- WP 446 Steel Equal Tee in Qatar
- UNS S44600 End Cap
- ASME SA403 Concentric Reducer
- SS S44600 Seamless Fitting
- Stainless Steel 446 45 Elbow
- SS 446 Pipe Bends
Countries We Export to
Nickel Super Alloys manufactures and exports Stainless Steel 446 Pipe Fittings to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia
Cities We Deliver to
Nickel Super Alloys manufactures and exports Stainless Steel 446 Pipe Fittings to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo