Inconel 601 Pipe & Tubes
ASTM B163 Alloy 601 Seamless Tubing, Inconel 601 Seamless Tubes, Inconel UNS N06601 Tubing, Inconel NCF 601 Tubes, Inconel 601 Polish Pipe, Inconel 601 Cold Rolled Coiled Tube Manufacturer in Mumbai,India.
Nickel Super Alloys is one of the prominent manufacturers and exporters of Inconel Alloy 601 Pipes and Tubes, which has high strength and good workability. Inconel 601 Seamless Pipes is a general-purpose engineering material for applications that require resistance to heat and corrosion. Inconel 601 Welded Tubes stands out due to its resistance to high temperature oxidation. Inconel 601 EFW Pipes is highly resistant to oxidation through 2200 Degree F. An addition of aluminum in Inconel 601 ERW Tubes gives outstanding resistance to oxidation and other forms of high temperature corrosion. Inconel 601 EFW Pipes are strengthened by performing solid-solution hardening, precipitation hardening and work hardening. Inconel 601 Round Tubes retains good strength at elevated temperatures.
Inconel 601 Square Pipes also has high mechanical properties at elevated temperatures. Popular as an engineering material, Inconel 601 Rectangular Tubes is perfect for applications that demand resistance to heat and corrosion. We are the well-known supplier and stockiest of industrial Inconel 601 Electropolish Pipes with required test certificates for best end products. The outstanding characteristic of Inconel 601 Hallow Tubes is its resistance to high-temperature oxidation. Inconel 601 Hexagonal Pipes is used for petrochemical and other process equipment; along with for gas-turbine components. Inconel 601 Bush Hex Tubes is also used for industrial furnaces and radiant tubes. Inconel UNS N06601 Pipes is a construction alloy for heat treat furnace fixtures and components such as annealing tubes and muffles.
Inconel WERKSTOFF NR. 2.4851 Pipe, 601 Inconel Heat exchanger Tube, ASTM B516 Inconel 601 Pipe, 601 Inconel Tubing, ASTM B163 Inconel 601 Pipe & Tube, Inconel Alloy 601 Pipe & Tubes, Suppliers in India.
Key Charactristic:
- Corrosion resistance
- Resistance to oxidation and sulfidation
- Cryogenic strength
- Resistance to abrasion and erosion
- Surface finish
- Magnetic properties
- Ductility
- Elevated temperature strength
- Stability of properties in service
- Suitability for intended fabrication techniques
Inconel 601 Pipe & Tubes Specifications
| Grade | Inconel 601 |
| Standard | ASTM B167, ASTM B751, ASTM B775, ASTM B829 |
| Inconel 601 Seamless Pipes | 1/4" NB To 6" NB |
| Inconel 601 Welded / ERW Pipes | 1" NB To 16" NB |
| Form | Round, Square, Rectangular, Hydraulic Etc |
| Schedule | SCH20, SCH30, SCH40, STD, SCH80, XS, SCH60, SCH80, SCH120, SCH140, SCH160, XXS |
| Length | Single Random, Double Random & Cut Length. |
| Type | Seamless / ERW / Welded / Fabricated / EFW |
| End | Plain End, Beveled End, Treaded |
| Standard | Inconel 601 |
| UNS | N06601 |
| DIN | 17751 |
| ISO | 6207 |
| WERKSTOFF NR. | 2.4851 |
Inconel 601 Pipe & Tubes Chemical Composition
| Ni | Cr | Al | C | Mn | Si | Fe |
|---|---|---|---|---|---|---|
| 61.5 | 22.5 | 1.4 | .05 | .3 | .2 | 14 |
Inconel 601 Pipe & Tubes Mechanical Properties
| Tensile (psi) | .2% Yield (psi) | Elongation (%) |
|---|---|---|
| 80,000 | 30,000 | 35 |
Other Types of Inconel 601 Pipe & Tubes
- SB751 Inconel Welded Tubes Supplier in UAE
- SB775 Rectangular Seamless Pipes Manufacturer in India
- Inconel 601 Round Pipe
- ASTM SB829 Inconel Capillary Tube
- Inconel SB775 U Shaped Tubing
- DIN 2.4851 Round Tubing
- UNS N06601 Hexagonal Pipe Distributors
- Alloy 601 Electropolish ERW Pipes
- Inconel 601 Fabricated Pipes
- Inconel 601 Round Pipe
- 601 Alloy Seamless Pipes Exporter in Russia
- Inconel 601 Pipes
- Alloy UNS N06601 Welded Pipes Supplier in Poland
- ASTM B167 Alloy 601 Pipes
- Alloy 601 Round Pipe in Qatar
- 601 Inconel ERW Pipes
- ASTM B751 Alloy 600 Pipe
- Inconel N06601 EFW Pipes
- Inconel 601 Heat Ex-changer Tubes
- UNS N06601 Inconel 601 Coiled Seamless Tubing
Countries We Export to
Nickel Super Alloys manufactures and exports Inconel 601 Pipes & Tubes to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia
Cities We Deliver to
Nickel Super Alloys manufactures and exports Inconel 601 Pipes & Tubes to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo