ASTM A106 GR B/C Carbon Steel Pipe & Tubes
ASTM A106 Welded Pipes & Tubes, ASTM A 106 GR. C Square Pipes, ASTM A 106 Grade B Rectangular Welded Pipes, A106 GR. B Carbon Seamless Pipe, ASTM A 106 GR. C Round Tubes Manufacturer in Mumbai,India.
Nickel Super Alloys is asupplier of ASTM A106 GR. B-C Carbon Steel Pipes & Tubes, which are provided as per the client specified. We are engaged in offering a high quality ASTM A106 GR. B Carbon Steel Seamless Pipes, which are offered at reasonable prices. We are a noteworthy trader and supplier of high grade of ASME SA106 GR. C Carbon Steel Welded Tubes, which is manufactured at our end using the supreme class component in line with international standard to ensure flawlessness at the users’ end. ASTM A106 GR. B Carbon Steel EFW Pipes has features like Dimensional accuracy, Durable, High strength, and more.
Our company is widely appreciated in offering ASME SA106 GR. C Carbon Steel ERW Tubes to the clients, which is manufactured from high grade quality raw material under the supervision of the professionals. ASTM A106 GR. B Carbon Steel Round Pipes are further offered to our clients as per their details, specifications and industry requirements. For us, quality serves as the most important factor for customers- so we ensure that our ASME SA106 GR. C Carbon Steel Square Tubes are made of the highest quality stainless steel to ensure your job is done and what’s more- at the best possible prices. ASTM A106 GR. B Carbon Steel Rectangular Pipes is processed precisely with both national & international quality standards under the direction of our proficient professionals.
ASTM A 106 ERW Tubes, A 106 GR B, A 106 GR C Carbon Steel Pipes & Tubes, ASTM A 106 Gr C ERW Tubing, ASTM A 106 Grade B / Grade C Seamless Tubing, ASTM A 106 Grade C EFW Tubing, Suppliers in India.
Key Charactristic:
- Corrosion resistance
- Resistance to oxidation and sulfidation
- Cryogenic strength
- Resistance to abrasion and erosion
- Surface finish
- Magnetic properties
- Ductility
- Elevated temperature strength
- Stability of properties in service
- Suitability for intended fabrication techniques
ASTM A106 GR B/C Carbon Steel Pipe & Tubes Specifications
| Grade | ASTM A106 Gr. B Carbon Steel |
| Size | 1/4” NB to 30” NB |
| Standard | ASTM A106, ASME SA106 |
| Form | Round, Square, Rectangular, Hydraulic Etc |
| Schedule | SCH20, SCH30, SCH40, STD, SCH80, XS, SCH60, SCH80, SCH120, SCH140, SCH160, XXS |
| Length | Single Random, Double Random & Cut Length. |
| Type | Seamless - Hot Rolled / Cold Drawn |
| End | Plain Ends, Beveled Ends and Coupling |
ASTM A106 GR B/C Carbon Steel Pipe & Tubes Chemical Composition
| Chemical Composition (%) | ||||||||||
| Grade | C(Max) | Mn | Si(Min) | Cu(Max) | Ni(Max) | Cr(Max) | Mo(Max) | V(Max) | P(Max) | S(Max) |
| B | 0.3 | 0.29~1.06 | 0.1 | 0.4 | 0.4 | 0.4 | 0.15 | 0.08 | 0.035 | 0.035 |
| Grade A | Grade B | Grade C | |
| Carbon max. % | 0.25 | 0.30 | 0.35 |
| *Manganese % | 0.27 to 0.93 | *0.29 to 1.06 | 0.29 to 1.06 |
| Phosphorous, max. % | 0.035 | 0.035 | 0.035 |
| Sulfur, max. % | 0.035 | 0.035 | 0.035 |
| Silicon, min.% | 0.10 | 0.10 | 0.10 |
| Chrome, max. % | 0.40 | 0.40 | 0.40 |
| Copper, max. % | 0.40 | 0.40 | 0.40 |
| Molybdenum, max. % | 0.15 | 0.15 | 0.15 |
| Nickel, max. % | 0.40 | 0.40 | 0.40 |
| Vanadium, max.% | 0.08 | 0.08 | 0.08 |
ASTM A106 GR B/C Carbon Steel Pipe & Tube Mechanical Properties
| Degree of Bend | Diameter of Mandrel | ||
| For Normal A106 Uses | 90 | 12 x nom dia. of pipe | |
| For Close Coiling | 180 | 8 x nom dia. of pipe |
Other Types of ASTM A106 GR B/C Carbon Steel Pipe & Tubes
- ASTM A 106 Gr C Welded Tubes Supplier in UAE
- ASTM A106 Welded Pipes & Tubes Manufacturer in India
- A106 Gr B Carbon Steel Capillary Tube
- ASTM A106 GR. B / C CS Pipes & Tubes
- Carbon Steel Seamless Rectangular Pipes
- ASTM A 106 Gr C ERW Tubing
- Carbon A106 Gr. B Pipes
- Carbon A106 Gr B Welded Pipes
- A106 Gr. C Carbon Steel Seamless Pipes
- CS A106 Grade B EFW Pipe
- ASTM A 106 Grade C Seamless Square Tubes Exporter in Russia
- ASTM A53 ERW CS Tubing
- A106 GR. C U Shaped Tubing Supplier in Poland
- A106 Gr B Carbon Steel Welded Tubing
- ASTM A106 Gr B Carbon Polished Pipe in Qatar
- A106 Gr. B CS Rectangular Pipe
- ASTM A106 Gr B Carbon LSAW Pipes
- A106 Gr. B Carbon Fabricated Pipes
- A106 GR. B Seamless pipe
- A106 GR. B Carbon Round Pipes
Countries We Export to
Nickel Super Alloys manufactures and exports ASTM A106 Gr B Pipe to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia
Cities We Deliver to
Nickel Super Alloys manufactures and exports ASTM A106 Gr B Pipe to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo