Inconel 601 Pipe Fittings
ASTM B366 Inconel 601 Pipe Fitting, 601 Alloy Seamless Pipe Fitting, ASME B16.28 Alloy 601 Short & Long Radius Elbow, Inconel 601 Eccentric & Concentric Reducer, Werkstoff Nr. 2.4851 Alloy 601 Unequal Tee Manufacturer in Mumbai,India.
Nickel Super Alloys is one of the prominent manufacturers and exporters of Inconel Alloy 601 Butt Weld Pipe Fittings, which is a solid solution nickel chromium heat resisting alloy. Inconel 601 Elbow Pipe Fittings is used for heat-treating equipment such as muffles, baskets, and retorts. Inconel 601 Tee Pipe Fittingsis also used for themocouple tubes and heat treatment equipment. Inconel 601 Cross Pipe Fittingsalso has high mechanical properties at elevated temperatures. An outstanding characteristic of Inconel 601 Reducer Pipe Fittings is its resistance to high-temperature oxidation. Inconel 601 Bend Pipe Fittings remains highly resistant to oxidation through 2200 Degree F. Inconel 601 Stub End Pipe Fittings also have good resistance to aqueous corrosion and have high mechanical strength.
Inconel 601 End Cap Pipe Fittings develops a tightly adherent oxide scale which resists spalling even under severe thermal cycling. Inconel 601 Dish Cap Pipe Fittings has excellent metallurgical stability and a high resistance to carburization. Inconel 601 Lateral Tee Pipe Fittings has outstanding resistance to oxidation & other forms of high temperature corrosion. Inconel 601 Concentric Reducer Pipe Fittings have good creep and oxidation resistance. Inconel 601 Eccentric Reducer Pipe Fittings was designed to with stand high temperature exposure and severe corrosive conditions. Inconel 601 Equal Tee Pipe Fittings has good aqueous corrosion resistance. Inconel 601 Unequal Tee Pipe Fittings gives outstanding performance at temperatures up to about 1200 Degree C. You can order Inconel UNS N06601 Pipe Fittings in small and large quantities as per your need.
Alloy 601 Concentric Reducer, Inconel 601 Elbow, Inconel 601 Short & Long Stub End, Inconel Alloy 601 Pipe Bend, UNS N06601 End Cap & Dish Cap, Inconel Alloy 601 Equal Tee, Alloy 601 Fitting Cross, Suppliers in India.
Key Charactristic:
- Corrosion resistance
- Resistance to oxidation and sulfidation
- Cryogenic strength
- Resistance to abrasion and erosion
- Surface finish
- Magnetic properties
- Ductility
- Elevated temperature strength
- Stability of properties in service
- Suitability for intended fabrication techniques
Inconel 601 Pipe Fittings Specifications
| Grade | Inconel Alloy 601 / UNS N06601 |
| Standard | ASTM B366, ASME SB366 |
| Dimensions | ASME B16.28, ASME/ANSI B16.9, MSS-SP-43 |
| Inconel 601 Seamless Fittings | 1/2" NB - 10" NB |
| Inconel 601 Welded Fittings | 1/2" NB - 48" NB |
| Form | 90 Elbow, 45 Elbow, Long Radius Elbow, Short Radius Elbow, Concentric Reducer, Eccentric Reducer, Equal Tee, Unequal Tee, Lateral Tee, Cross, Bends 1.5d, 3d, 5d, 10d, U bend, 180 Deg Bend, Short Stub End, Long stub end, End Cap, Dish Cap |
| Schedule | SCH 5 To SCH XXS |
| Wall Thickness | from 2 to 40 mm |
| Type | Seamless / Welded / Fabricated |
| Standard | Inconel 601 |
| UNS | N06601 |
| DIN | 17751 |
| ISO | 6207 |
| WERKSTOFF NR. | 2.4851 |
Inconel 601 Pipe Fittings Chemical Composition
| Grade | C | Mn | Si | S | Cu | Fe | Ni | Cr |
| Inconel 601 |
0.15 max | 1.00 max | 0.50 max | 0.015max | 1.0 max | balance | 58.0-63.0 | 21.0-25.0 |
Inconel 601 Pipe Fittings Mechanical Properties
| Element | Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
| Inconel 601 |
8.1 g/cm3 | 1411 °C (2571 °F) | Psi – 80,000 , MPa – 550 | Psi – 30,000 , MPa – 205 | 30 % |
Other Types of Inconel 601 Pipe Fittings
- Inconel 601 Buttweld Tee Supplier in UAE
- UNS N06601 Cross Manufacturer in India
- Inconel 601 Butwteld Tee
- DIN 2.4851 45 deg.Elbow
- DIN 2.4851 Buttweld Pipe Fittings
- Inconel 601 Short Radius Elbow
- UNS N06601 Ecentric Reducer Distributors
- Inconel 601 Buttweld Pipe Fitting
- ASME SB366 Stub End
- 601 Inconel Concentric Reducer
- ASTM B366 Inconel 601 Long Radius Elbow Exporter in Russia
- Inconel 601 U Bend
- Inconel 601 Stub End Supplier in Poland
- 601 Inconel Short Radius Elbow
- Inconel 601 Equal Tee in Qatar
- UNS N06601 End Cap
- ASME SB366 Concentric Reducer
- Inconel 601 Seamless Fitting
- Inconel 601 45 Deg Elbow
- Inconel 601 Pipe Bends
Countries We Export to
Nickel Super Alloys manufactures and exports Inconel 601 Pipe Fittings to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia
Cities We Deliver to
Nickel Super Alloys manufactures and exports Inconel 601 Pipe Fittings to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo