Hastelloy C276 Threaded Forged Fittings
Hastelloy C276 Forged Threaded 90 Deg. Elbow, Hastelloy C276 Threaded Tee, UNS N10276 Threaded Cross, DIN 2.4819 Threaded Forged Cap Manufacturer in Mumbai, India.
Nickel Super Alloys is a known supplier and exporter of Hastelloy Alloy C276 Threaded Forged Fittings, which is suitable for most chemical process applications in an as welded condition. The high molybdenum content of Hastelloy C276 Threaded Elbow Forged Fittings provides the alloy with its excellent resistance to pitting and crevice corrosion. The high nickel and molybdenum contents make Hastelloy C276 Threaded Tee Forged Fittings especially resistant to pitting and crevice corrosion in reducing environments. We have track record of proven performance for Hastelloy C276 Threaded Cross Forged Fittings in a vast number of corrosive chemicals. Hastelloy C276 Threaded Cap Forged Fittings is often used for stack-gas re-heaters, reaction vessels, heat exchangers, and evaporators.
Hastelloy C276 Threaded Coupling Forged Fittings is used in most industrial settings where aggressive chemical environments are present and other alloys have failed. Parts made from Hastelloy C276 Threaded Bend Forged Fittings blends tend to find good use across a wide range of chemical applications. Hastelloy C276 Threaded Union Forged Fittings maintains resistance to inter-granular attack in heat-affected zones of welded joints. Hastelloy C276 Threaded Bushing Forged Fittings exhibits good high temperature strength and moderate oxidation resistance. The combination of the high molybdenum and chromium content, along with the addition of tungsten, make Hastelloy C276 Threaded Plug Forged Fittings highly resistant to chloride SCC. Hastelloy C276 Threaded Hex Plus Forged Fittings is one of the few materials that withstand the corrosive effects of wet chlorine gas, chlorine dioxide and hypochlorite.
Hastelloy C276 Threaded Cap, Alloy C276 Threaded Bend, UNS N10276 Threaded Weld Cross, Hastelloy C276 Threaded Bushing, DIN 2.4819 Threaded Coupling, Hastelloy C276 Threaded Union Suppliers in India.
Key Charactristic:
- Corrosion resistance
- Resistance to oxidation and sulfidation
- Cryogenic strength
- Resistance to abrasion and erosion
- Surface finish
- Magnetic properties
- Ductility
- Elevated temperature strength
- Stability of properties in service
- Suitability for intended fabrication techniques
Hastelloy C276 Threaded Forged Fittings Specifications
| Grade | Hastelloy C276 | UNS N10276 |
| Standard | ASTM B564 & ASME SB564 |
| Dimensions | ASME 16.11, MSS SP-79, 83, 95, 97, BS 3799 |
| Size | 1/8” NB to 4” NB (Socketweld & Screwed-Threaded) |
| Class | 2000 LBS, 3000 LBS, C2760 LBS, 9000 LBS |
| Form | Threaded 45 deg Elbow, Threaded 90 deg Elbow, Threaded Tee, Threaded Cross, Threaded Cap, Threaded Bend, Threaded Coupling, Threaded Union , Threaded Bushing, Plug, Hex Plus, Hexagonal Plus, Lateral Tee. |
| Type | Threaded Forged Fittings |
| Standard | Hastelloy C276 |
| EN | NiMo16Cr15W |
| UNS | N10276 |
| OR | ЭП760 |
| JIS | NW 0276 |
| GOST | ХН65МВУ |
| AFNOR | NFE30C20DUM |
| WERKSTOFF NR. | 2.4819 |
| BS | - |
Hastelloy C276 Threaded Forged Fittings Chemical Composition
| Grade | C | Mn | Si | S | Co | Ni | Cr | Fe | Mo | P |
| C276 | 0.01 max | 1.00 max | 0.08 max | 0.03 max | 2.50 max | 50.99 min* | 14.50 – 16.50 | 4.00 – 7.00 | 15.0 – 17.0 | 0.04 max |
Hastelloy C276 Threaded Forged Fittings Mechanical Properties
| Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
| 8.89 g/cm3 | 1370 °C (2500 °F) | Psi – 1,15,000 , MPa – 790 | Psi – 52000 , MPa – 355 | 40 % |
Other Types of Hastelloy C276 Threaded Forged Fittings
- Hastelloy C276 Forged Elbow Supplier in UAE
- Hastelloy C276 Equal Tee Manufacturer in India
- Hastelloy C276 Threaded Cross
- UNS N10276 Threaded Union
- UNS N10276 Hexagonal Plug
- DIN 2.4819 Threaded Hex Plug
- DIN 2.4819 45 Deg Threaded Elbow Distributors
- Hastelloy C276 Threaded Bushing
- Hastelloy C276 Threaded Lateral Tee
- Alloy C276 Alloy Threaded Cross
- Hastelloy C276 Threaded Coupling Exporter in Russia
- Alloy C276 Threaded Tees
- UNS N10276 45 deg Elbow Supplier in Poland
- UNS N10276 Threaded 90 deg Elbow
- DIN 2.4819 Threaded Cap in Qatar
- DIN 2.4819 Threaded Bend Flanges
- Hastelloy C276 Threaded Union
- Alloy C276 Threaded Bushing
- Hastelloy C276 Lateral Tee
- Hastelloy C276 Threaded Cross
Countries We Export to
Nickel Super Alloys manufactures and exports Hastelloy C276 Threaded Forged Fittings to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia
Cities We Deliver to
Nickel Super Alloys manufactures and exports Hastelloy C276 Threaded Forged Fittings to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo