Super Duplex Steel UNS S32750 / S32760 Threaded Forged Fittings
Super Duplex Steel UNS S32750 / S32760 Forged Threaded 90 Deg. Elbow, UNS S32750 Threaded Tee, UNS S32760 Threaded Cross, DIN 1.4410 Threaded Forged Cap Manufacturer in Mumbai, India.
Nickel Super Alloys is one of the notable exporters of Super Duplex Steel S32750 / S32760 Threaded Forged Fittings, which has superior localized corrosion resistance. Super Duplex S32750 Threaded Elbow Forged Fittings is suitable for service in highly corrosive conditions and where high strength is required. Super Duplex S32760 Threaded Tee Forged Fittingsisused for upstream production of firefighting systems,oil & gas fluids, etc. In addition, Super Duplex S32750 Threaded Cross Forged Fittings offers high resistance to crevice corrosion and stress corrosion cracking. Super Duplex S32760 Threaded Cap Forged Fittings is specially designed to resist pure sulfuric acid. Super Duplex S32750 Threaded Coupling Forged Fittings has a higher molybdenum and chromium content which gives the material greater corrosion resistance.
The high chromium and molybdenum content of Super Duplex S32760 Threaded Bend Forged Fittings makes it extremely resistant to uniform corrosion by organic acids. Super Duplex S32750 Threaded Union Forged Fittings is also resistant to chloride SCC, to erosion corrosion. Super Duplex S32760 Threaded Bushing Forged Fittings provides excellent resistance to inorganic acids, especially those containing chlorides. The structure provides Super Duplex S32750 Threaded Plug Forged Fittings with exceptional resistance to chloride stress corrosion cracking. Supplied in the annealed condition, Super Duplex S32760 Threaded Hexagonal Plus Forged Fittingsachieves yield strengths, greater than most austenitic and duplex stainless steel grades. These Super Duplex S32750 Threaded Lateral Tee Forged Fittingswere developed for applications in aggressive chloride environments.
Super Duplex Steel UNS S32750 Threaded Cap, UNS S32760 Threaded Bend, UNS S32750 Threaded Weld Cross, UNS S32760 Threaded Bushing, DIN 1.4410 Threaded Coupling, UNS S32750 Threaded Union Suppliers in India.
Key Charactristic:
- Corrosion resistance
- Resistance to oxidation and sulfidation
- Cryogenic strength
- Resistance to abrasion and erosion
- Surface finish
- Magnetic properties
- Ductility
- Elevated temperature strength
- Stability of properties in service
- Suitability for intended fabrication techniques
Super Duplex Steel UNS S32750 / S32760 Threaded Forged Fittings Specifications
| Grade | Super Duplex S32750 / S32760 |
| Standard | ASTM A182 & ASME SA182 |
| Dimensions | ASME 16.11, MSS SP-79, 83, 95, 97, BS 3799 |
| Size | 1/8” NB to 4” NB |
| Class | 2000 LBS, 3000 LBS, 6000 LBS, 9000 LBS |
| Form | Threaded 45 deg Elbow, Threaded 90 deg Elbow, Threaded Tee, Threaded Cross, Threaded Cap, Threaded Bend, Threaded Coupling, Threaded Union , Threaded Bushing, Plug, Hex Plus, Hexagonal Plus, Lateral Tee. |
| Type | Threaded Forged Fittings |
| STANDARD | WERKSTOFF NR. | UNS | JIS | BS | GOST | AFNOR | EN |
| Super Duplex S32750 / S32760 | 1.4410 | S32750 / S32760 | - | - | - | - | - |
UNS S32750 / S32760 Threaded Forged Fittings Chemical Composition
| Grade | C | Mn | Si | P | S | Cr | Mo | Ni | N | Fe |
| S32750 | 0.030 max | 1.20 max | 0.80 max | 0.035 max | 0.020 max | 24.00 – 26.00 | 3.00 – 5.00 | 6.00 – 8.00 | 0.24 – 0.32 | 58.095 min |
| S32760 | 0.05 max | 1.00 max | 1.00 max | 0.030 max | 0.010 max | 24.00 – 26.00 | 3.00 – 4.00 | 6.00 – 8.00 | 0.20 – 0.30 | 57.61 min |
UNS S32750 / S32760 Threaded Forged Fittings Mechanical Properties
| Grades | Density (g/cm 3) | Density (lb/in 3) | Melting Point (°C) | Melting Point (°F) |
| S32750 / S32760 | 7.8 | 0.281 | 1350 | 2460 |
Other Types of UNS S32750 / S32760 Threaded Forged Fittings
- Super Duplex Steel UNS S32750 Forged Elbow Supplier in UAE
- Super Duplex Steel UNS S32760 Equal Tee Manufacturer in India
- UNS S32750 Threaded Cross
- UNS S32760 Threaded Union
- UNS S32750 Hexagonal Plug
- DIN 1.4410 Threaded Hex Plug
- DIN 1.4410 45 Deg Threaded Elbow Distributors
- A182 Super Duplex Steel F57 Threaded Bushing
- UNS S32750 Threaded Lateral Tee
- UNS S32760 Alloy Threaded Cross
- Super Duplex Steel UNS S32750 Threaded Coupling Exporter in Russia
- Super Duplex Steel UNS S32760 Threaded Tees
- UNS S32750 45 deg Elbow Supplier in Poland
- UNS S32760 Threaded 90 deg Elbow
- DIN 1.4410 Threaded Cap in Qatar
- DIN 1.4410 Threaded Bend Flanges
- Super Duplex UNS S32750 Threaded Union
- Super Duplex UNS S32760 Threaded Bushing
- Super Duplex 2507 Lateral Tee
- Super Duplex 2507 Threaded Cross
Countries We Export to
Nickel Super Alloys manufactures and exports Super Duplex Steel UNS S32750 / S32760 Threaded Forged Fittings to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia
Cities We Deliver to
Nickel Super Alloys manufactures and exports Super Duplex Steel UNS S32750 / S32760 Threaded Forged Fittings to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo