Copper Nickel 90/10 Threaded Forged Fittings
Copper Nickel 90/10 Forged Threaded 90 Deg. Elbow, UNS C70600 Threaded Tee, Cupro Nickel 90/10 Threaded Cross, DIN 2.0872 Threaded Forged Cap Manufacturer in Mumbai, India.
Nickel Super Alloys is a renowned distributor of Copper Nickel 90 / 10 Threaded Forged Fittings, which has nominal temperature coefficient of electric resistance. Cupro Nickel 90 / 10 Threaded Elbow Forged Fittings offer excellent resistance to stress corrosion, erosion, and bio-fouling in seawater and brackish water. Cu-Ni 90 / 10 Threaded Tee Forged Fittings also have important additions of iron and manganese which are necessary to maintain good corrosion resistance. Copper Nickel 90 / 10 Threaded Cross Forged Fittings high oxidation resistance and stress corrosion cracking resistance. Additions of iron significantly improve the resistance of Cupro Nickel 90 / 10 Threaded Cap Forged Fittings to erosion corrosion in flowing seawater and other aggressive waters.
Cu-Ni90 / 10 Threaded Coupling Forged Fittingsa re used in heat exchangers and condensers in seawater systems, as well as for marine hardware. Copper Nickel 90 / 10 Threaded Bend Forged Fittings are also immune to chloride and sulphide stress corrosion cracking. Cupro Nickel 90 / 10 Threaded Union Forged Fittings have the inherent biofouling resistance of the alloys with the aim of learning from past experiences. Cu-Ni 90 / 10 Threaded Bushing Forged Fittings can be fabricated by both hot and cold-working procedures, and is readily weldable. Copper Nickel 90 / 10 Threaded Plug Forged Fittingshas excellent erosion and impingement due to turbulent water containing air bubbles and silt flowing at high velocities.
Copper Nickel 90/10 Threaded Cap, CU-Ni 90/10 Threaded Bend, CU-Ni 90/10 Threaded Weld Cross, UNS C70600 Threaded Bushing, DIN 2.0872 Threaded Coupling, Cupro Nickel 90/10 Threaded Union Suppliers in India.
Key Charactristic:
- Corrosion resistance
- Resistance to oxidation and sulfidation
- Cryogenic strength
- Resistance to abrasion and erosion
- Surface finish
- Magnetic properties
- Ductility
- Elevated temperature strength
- Stability of properties in service
- Suitability for intended fabrication techniques
Copper Nickel 90/10 Threaded Forged Fittings Specifications
| Grade | Copper Nickel 90-10 | UNS C70600 |
| Standard | ASTM B122, ASTM B171, ASTM B466, ASTM B467 |
| Dimensions | ASME 16.11, MSS SP-79, 83, 95, 97, BS 3799 |
| Size | 1/8” NB to 4” NB (Socketweld & Screwed-Threaded) |
| Class | 90-100 LBS, 3000 LBS, 90-100 LBS, 9000 LBS |
| Form | Threaded 45 deg Elbow, Threaded 90 deg Elbow, Threaded Tee, Threaded Cross, Threaded Cap, Threaded Bend, Threaded Coupling, Threaded Union , Threaded Bushing, Plug, Hex Plus, Hexagonal Plus, Lateral Tee. |
| Type | Threaded Forged Fittings |
| Standard | Copper Nickel 90-10 |
| UNS | C70600 |
| WERKSTOFF NR. | 2.0872 |
Copper Nickel 90/10 Threaded Forged Fittings Chemical Composition
| Grade | Cu | Mn | Pb | Ni | Fe | Zn |
| Cupro Nickel 90/10 | 88.6 min | 1.0 max | 0.05 max | 9-11 max | 1.8 max | 1 max |
Copper Nickel 90/10 Threaded Forged Fittings Mechanical Properties
| Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
| 0.323 lb/in3 at 68 F | 2260 F | 50000 psi | 20000 psi | 30 % |
Other Types of Copper Nickel 90/10 Threaded Forged Fittings
- Copper Nickel 90/10 Forged Elbow Supplier in UAE
- Cupro Nickel 90/10 Equal Tee Manufacturer in India
- Cu-Ni 90/10 Threaded Cross
- UNS C70600 Threaded Union
- UNS C70600 Hexagonal Plug
- DIN 2.0872 Threaded Hex Plug
- DIN 2.0872 45 Deg Threaded Elbow Distributors
- Cu-Ni 90/10 Threaded Bushing
- Copper Nickel 90/10 Threaded Lateral Tee
- Cupro Nickel 90/10 Alloy Threaded Cross
- Copper Nickel 90/10 Threaded Coupling Exporter in Russia
- Cupro Nickel 90/10 Threaded Tees
- UNS C70600 45 deg Elbow Supplier in Poland
- UNS C70600 Threaded 90 deg Elbow
- DIN 2.0872 Threaded Cap in Qatar
- DIN 2.0872 Threaded Bend Flanges
- Cu-Ni 90/10 Threaded Union
- Cu-Ni 90/10 Threaded Bushing
- Copper Nickel 90/10 Lateral Tee
- Cupro Nickel 90/10 Threaded Cross
Countries We Export to
Nickel Super Alloys manufactures and exports Copper Nickel 90/10 Threaded Forged Fittings to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia
Cities We Deliver to
Nickel Super Alloys manufactures and exports Copper Nickel 90/10 Threaded Forged Fittings to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo