Hastelloy B3 Socket Weld Forged Fittings
Hastelloy B3 Socket Weld 90 Deg. Elbow, Hastelloy B3 Socket Weld Tee, UNS N10675 Socket Weld Cross, DIN NR. 2.4600 Socket Weld Forged Cap Manufacturer in Mumbai, India.
Nickel Super Alloys is a known manufacturer and supplier of Hastelloy Alloy B3 Socket Weld Forged Fittings, which resists other vigorously corrosive agents extremely well. Hastelloy B3 Socket Weld Elbow Forged Fittings is a nickel-molybdenum alloy with excellent resistance to pitting and corrosion. In addition, additional uses for Hastelloy B3 Socket Weld Tee Forged Fittings include some comparative corrosion resistance media, data ,concentrations and temperatures. Distinguishing feature of Hastelloy B3 Socket Weld Cross Forged Fittings is its ability to maintain excellent ductility during transient exposures to intermediate temperatures. Also, Hastelloy B3 Socket Weld Cap Forged Fittingsis able to withstand fluoride-bearing media and concentrated sulfuric acid, both of which result in damage to zirconium alloys.
Hastelloy B3 Socket Weld Coupling Forged Fittingsis used in numerous chemical process industry (CPI) applications. Hastelloy B3 Socket Weld Union Forged Fittings has excellent corrosion resistance to hydrochloric acid at all concentrations and temperatures. The improved thermal stability of Hastelloy B3 Socket Weld Plug Forged Fittings minimizes the problems associated with fabrication of B2 alloy components. Hastelloy B3 Socket Weld Lateral Tee Forged Fittings has greater ductility than B-2 alloy during and following various thermal cycling conditions. Likewise, Hastelloy UNS N10675 Socket Weld Forged Fittings does not withstand wet chlorine gas or hypochlorite bleach. Therefore, Hastelloy WNR 2.4600 Socket Weld Forged Fittings is used in conjunction with iron or copper piping in a system containing hydrochloric acid.
Hastelloy B3 Socket Weld Cap, Hastelloy B3 Socket Weld Bend, Hastelloy B3 Socket Weld Cross, Hastelloy B3 Socket Weld Bushing, UNS N10675 Socket Weld Coupling, ASTM B564 Hastelloy B3 Socket Weld Union Suppliers in India.
Key Charactristic:
- Corrosion resistance
- Resistance to oxidation and sulfidation
- Cryogenic strength
- Resistance to abrasion and erosion
- Surface finish
- Magnetic properties
- Ductility
- Elevated temperature strength
- Stability of properties in service
- Suitability for intended fabrication techniques
Hastelloy B3 Socket Weld Forged Fittings Specifications
| Grade | Hastelloy B3 | UNS N10675 |
| Standard | ASTM B564 & ASME SB564 |
| Dimensions | ASME 16.11, MSS SP-79, 83, 95, 97, BS 3799 |
| Size | 1/8” NB to 4” NB |
| Class | 2000 LBS, 3000 LBS, B30 LBS, 9000 LBS |
| Form | Socket weld 45 deg Elbow, Socket weld 90 deg Elbow, Socket weld Tee, Socket weld Cross, Socket weld Cap, Socket weld Bend, Socket weld Coupling, Socket weld Union , Socket weld Bushing, Plug, Hex Plus, Hexagonal Plus, Lateral Tee. |
| Type | Socket weld Forged Fittings |
| Standard | Hastelloy B3 |
| UNS | N10675 |
| WERKSTOFF NR. | - |
Hastelloy B3 Socket Weld Forged Fittings Chemical Composition
| Grade | C | Mn | Si | P | S | Cu | Mo | Ni | Fe | Cr |
| Hastelloy B3 | 0.01 max | 3.00 max | 0.10 max | 0.04 max | 0.03 max | 0.20 max | 28.5 | 65 min | 15 | 1.50 max |
Hastelloy B3 Socket Weld Forged Fittings Mechanical Properties
| Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
Other Types of Hastelloy B3 Socket Weld Threaded Forged Fittings
- Hastelloy B3 Socket Weld Forged Elbow Supplier in UAE
- Hastelloy B3 Socket Weld Equal Tee Manufacturer in India
- Hastelloy B3 Socket Weld Cross
- Hastelloy B3 Socket Weld Union
- UNS N10675 Socket Weld Plug
- UNS N10675 Socket Weld Hex Plug
- DIN NR. 2.4600 45 Deg Socket Weld Elbow Distributors
- DIN NR. 2.4600 Socket Weld Bushing
- Hastelloy B3 Socket Weld Lateral Tee
- Hastelloy B3 Socket Weld Cross
- Hastelloy B3 Socket Weld Tees
- UNS N10675 45 deg Socket Weld Elbow Supplier in Poland
- UNS N10675 Socket Weld 90 deg Elbow
- DIN NR. 2.4600 Socket Weld Cap in Qatar
- DIN NR. 2.4600 Socket Weld Bend Flanges
- Hastelloy B3 Socket Weld Union
- Hastelloy B3 Socket Weld Bushing
- Hastelloy B3 Socket Weld Lateral Tee
- Hastelloy B3 Socket Weld Cross
Countries We Export to
Nickel Super Alloys manufactures and exports Hastelloy B3 Socket Weld Forged Fittings to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia
Cities We Deliver to
Nickel Super Alloys manufactures and exports Hastelloy B3 Socket Weld Forged Fittings to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo