Copper Nickel 90/10 Socket Weld Forged Fittings
Copper Nickel 90/10 Socket Weld 90 Deg. Elbow, Cu-Ni 90/10 Socket Weld Tee, UNS C70600 Socket Weld Cross, DIN NR. 2.0872 Socket Weld Forged Cap Manufacturer in Mumbai, India.
Nickel Super Alloys is a renowned distributor of Copper Nickel 90 / 10 Socket Weld Forged Fittings, which is a copper-nickel alloy that shows good resistant to stress corrosion.Cupro Nickel 90 / 10 Socket Weld Elbow Forged Fittings have excellent fabrication and welding properties, along with a high resistance to hydrogen embrittlement. Cu-Ni90 / 10 Socket Weld Tee Forged Fittings prevents stress corrosion cracking and pitting and crevice corrosion. Copper Nickel 90 / 10 Socket Weld Cap Forged Fittings have good fabricability and high inherent resistance to biofouling. Cupro Nickel 90 / 10 Socket Weld Coupling Forged Fittings has a small content of manganese which allows excellent resistance to sea- and brackish water. Other uses of Cu-Ni 90 / 10 Socket Weld Cross Forged Fittings include military equipment, electrical, chemical and petrochemical industries.
Copper Nickel 90 / 10 Socket Weld Union Forged Fittings ensures good commissioning and operational practices for future use. Cupro Nickel 90 / 10 Socket Weld Plug Forged Fittingsis not recommended for usage in heavily polluted water containing sewage and industrial wastes. Cu-Ni90 / 10 Socket Weld Lateral Tee Forged Fittings have corrosion resistance and inherent resistance to biofouling in salt water environments. Copper Nickel C70600 Socket Weld Forged Fittings has excellent resistance to corrosion in the atmosphere and in fresh water. Cupro nickel C70600 Socket Weld Forged Fittings contains small but significant amount of additions of iron and manganese.
Copper Nickel 90/10 Socket Weld Cap, Cu-Ni 90/10 Socket Weld Bend, Cupro Nickel 90/10 Socket Weld Cross, UNS C70600 Socket Weld Bushing, Cu-Ni 90/10 Socket Weld Coupling, Cupro Nickel 90/10 Socket Weld Union Suppliers in India.
Key Charactristic:
- Corrosion resistance
- Resistance to oxidation and sulfidation
- Cryogenic strength
- Resistance to abrasion and erosion
- Surface finish
- Magnetic properties
- Ductility
- Elevated temperature strength
- Stability of properties in service
- Suitability for intended fabrication techniques
Copper Nickel 90/10 Socket Weld Forged Fittings Specifications
| Grade | Copper Nickel 90-10 | UNS C70600 |
| Standard | ASTM B122, ASTM B171, ASTM B466, ASTM B467 |
| Dimensions | ASME 16.11, MSS SP-79, 83, 95, 97, BS 3799 |
| Size | 1/8” NB to 4” NB |
| Class | 90-100 LBS, 3000 LBS, 90-100 LBS, 9000 LBS |
| Form | Socket weld 45 deg Elbow, Socket weld 90 deg Elbow, Socket weld Tee, Socket weld Cross, Socket weld Cap, Socket weld Bend, Socket weld Coupling, Socket weld Union , Socket weld Bushing, Plug, Hex Plus, Hexagonal Plus, Lateral Tee. |
| Type | Socket weld Forged Fittings |
| Standard | Cu-Ni 90-10 |
| UNS | C70600 |
| WERKSTOFF NR. | 2.0872 |
Copper Nickel 90/10 Socket Weld Forged Fittings Chemical Composition
| Grade | Cu | Mn | Pb | Ni | Fe | Zn |
| Cupro Nickel 90/10 | 88.6 min | 1.0 max | 0.05 max | 9-11 max | 1.8 max | 1 max |
Copper Nickel 90/10 Socket Weld Forged Fittings Mechanical Properties
| Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
| 0.323 lb/in3 at 68 F | 2260 F | 50000 psi | 20000 psi | 30 % |
Other Types of Copper Nickel 90/10 Socket Weld Threaded Forged Fittings
- Copper Nickel 91/10 Socket Weld Forged Elbow Supplier in UAE
- Copper Nickel 91/10 Socket Weld Equal Tee Manufacturer in India
- Cu-Ni 91/10 Socket Weld Cross
- UNS C70600 Socket Weld Union
- UNS C70600 Socket Weld Plug
- Cu-Ni 91/10 Socket Weld Hex Plug
- DIN NR. 2.0872 45 Deg Socket Weld Elbow Distributors
- DIN NR. 2.0872 Socket Weld Bushing
- Cupro Nickel 90/10 Socket Weld Lateral Tee
- Cupro Nickel 90/10 Socket Weld Cross
- Copper Nickel 90/10 Socket Weld Tees
- Cupro Nickel 90/10 45 deg Socket Weld Elbow Supplier in Poland
- Cu-Ni 90/10 Socket Weld 90 deg Elbow
- DIN NR. 2.0872 Socket Weld Cap in Qatar
- DIN NR. 2.0872 Socket Weld Bend Flanges
- Copper Nickel 90/10 Socket Weld Union
- Cupro Nickel 90/10 Socket Weld Bushing
- Cu-Ni 90/10 Socket Weld Lateral Tee
- Cu-Ni 90/10 Socket Weld Cross
Countries We Export to
Nickel Super Alloys manufactures and exports Copper Nickel 90/10 Socket Weld Forged Fittings to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia
Cities We Deliver to
Nickel Super Alloys manufactures and exports Copper Nickel 90/10 Socket Weld Forged Fittings to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo