Hastelloy B2 Socket Weld Forged Fittings
Hastelloy B2 Socket Weld 90 Deg. Elbow, Hastelloy B2 Socket Weld Tee, UNS N10665 Socket Weld Cross, DIN NR. 2.4617 Socket Weld Forged Cap Manufacturer in Mumbai, India.
Nickel Super Alloys is one of the known supplier and exporter of Hastelloy Alloy B2 Socket Weld Forged Fittings, which can be used in the as-welded condition. Premature failure may occur if Hastelloy B2 Socket Weld Elbow Forged Fittings is used where iron or copper is present in a system containing hydrochloric acid. Hastelloy B2 Socket Weld Tee Forged Fittings has many different industrial applications, some of which include chemical process applications. Controlling other alloying elements such as iron and chromium in Hastelloy B2 Socket Weld Cap Forged Fittingshassolved other issues concerning fabricability. Because this alloy contains no significant chromium addition, Hastelloy B2 Socket Weld Cross Forged Fittings should NOT be used in oxidizing media.
Hastelloy B2 Socket Weld Coupling Forged Fittings exhibits good resistance to sulfuric acid, hydrogen chloride, and phosphoric acid. Hastelloy B2 Socket Weld Union Forged Fittings has good resistance to chloride-induced stress-corrosion cracking (SCC). Hastelloy B2 Socket Weld Plug Forged Fittings should not be used in the presence of oxidizing media. The primary function of Hastelloy B2 Socket Weld Lateral Tee Forged Fittings is that of effective survival under high-temperature. Hastelloy UNS N10665 Socket Weld Forged Fittings is anickel-base wrought alloy with excellent resistance tohydrochloric acid at allconcentrations and temperatures. Hastelloy WNR 2.4617 Socket Weld Forged Fittings should not be used where ferric or cupric salts are present as these salts may cause rapid corrosion failure.
Hastelloy B2 Socket Weld Cap, Hastelloy B2 Socket Weld Bend, Hastelloy B2 Socket Weld Cross, Hastelloy B2 Socket Weld Bushing, UNS N10665 Socket Weld Coupling, ASTM B564 Hastelloy B2 Socket Weld Union Suppliers in India.
Key Charactristic:
- Corrosion resistance
- Resistance to oxidation and sulfidation
- Cryogenic strength
- Resistance to abrasion and erosion
- Surface finish
- Magnetic properties
- Ductility
- Elevated temperature strength
- Stability of properties in service
- Suitability for intended fabrication techniques
Hastelloy B2 Socket Weld Forged Fittings Specifications
| Grade | Hastelloy B2 | UNS N10665 |
| Standard | ASTM B564 & ASME SB564 |
| Dimensions | ASME 16.11, MSS SP-79, 83, 95, 97, BS 3799 |
| Size | 1/8” NB to 4” NB |
| Class | 2000 LBS, 3000 LBS, B20 LBS, 9000 LBS |
| Form | Socket weld 45 deg Elbow, Socket weld 90 deg Elbow, Socket weld Tee, Socket weld Cross, Socket weld Cap, Socket weld Bend, Socket weld Coupling, Socket weld Union , Socket weld Bushing, Plug, Hex Plus, Hexagonal Plus, Lateral Tee. |
| Type | Socket weld Forged Fittings |
| Standard | Hastelloy B2 |
| UNS | N10665 |
| WERKSTOFF NR. | 2.4617 |
Hastelloy B2 Socket Weld Forged Fittings Chemical Composition
| Grade | C | Mn | Si | P | S | Co | Mo | Ni | Fe | Cr |
| Hastelloy B2 | 0.02 max | 1.00 max | 0.1 max | 0.04 max | 0.03 max | 1.00 max | 26.0-30.0 | Balance | 2.00 max | 20.00 – 22.50 |
Hastelloy B2 Socket Weld Forged Fittings Mechanical Properties
| Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
| 9.2 g/cm3 | 1370 °C (2500 ºF ) | Psi – 1,10,000 , MPa – 760 | Psi – 51000 , MPa – 350 | 40 % |
Other Types of Hastelloy B2 Socket Weld Threaded Forged Fittings
- Hastelloy B2 Socket Weld Forged Elbow Supplier in UAE
- Hastelloy B2 Socket Weld Equal Tee Manufacturer in India
- Hastelloy B2 Socket Weld Cross
- Hastelloy B2 Socket Weld Union
- UNS N10665 Socket Weld Plug
- UNS N10665 Socket Weld Hex Plug
- DIN NR. 2.4617 45 Deg Socket Weld Elbow Distributors
- DIN NR. 2.4617 Socket Weld Bushing
- Hastelloy B2 Socket Weld Lateral Tee
- Hastelloy B2 Socket Weld Cross
- Hastelloy B2 Socket Weld Tees
- UNS N10665 45 deg Socket Weld Elbow Supplier in Poland
- UNS N10665 Socket Weld 90 deg Elbow
- DIN NR. 2.4617 Socket Weld Cap in Qatar
- DIN NR. 2.4617 Socket Weld Bend Flanges
- Hastelloy B2 Socket Weld Union
- Hastelloy B2 Socket Weld Bushing
- Hastelloy B2 Socket Weld Lateral Tee
- Hastelloy B2 Socket Weld Cross
Countries We Export to
Nickel Super Alloys manufactures and exports Hastelloy B2 Socket Weld Forged Fittings to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia
Cities We Deliver to
Nickel Super Alloys manufactures and exports Hastelloy B2 Socket Weld Forged Fittings to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo