Copper Nickel 70/30 Threaded Forged Fittings
Copper Nickel 70/30 Forged Threaded 90 Deg. Elbow, UNS C71500 Threaded Tee, Cupro Nickel 70/30 Threaded Cross, DIN 2.0882 Threaded Forged Cap Manufacturer in Mumbai, India.
Nickel Super Alloys is a leading Manufacturer supplier of Copper Nickel 70 / 30 Threaded Forged Fittings, which have excellent cold working capability. Cupro Nickel 70 / 30 Threaded Elbow Forged Fittings has been used as an alternative to traditional steel brake lines, as it does not rust. Cu-Ni 70 / 30 Threaded Tee Forged Fittings falls into the moderate to poor machining ability category due to its durability. Copper Nickel 70 / 30 Threaded Cross Forged Fittings is readily cold worked, welded and fabricated without any special material considerations. Cupro Nickel 70 / 30 Threaded Cap Forged Fittings is very suitable and ideal for the marine or industrial industries.
Cu-Ni 70 / 30 Threaded Coupling Forged Fittings can be utilized up to 700 Degree F for ASME code heat exchangers and unfired pressure vessels. Copper Nickel 70 / 30 Threaded Bend Forged Fittings has high strength and excellent corrosion resistance. Cupro Nickel 70 / 30 Threaded Union Forged Fittings are resistant to impingement corrosion and prevent attack by alkali and acidic media. The corrosion resistance and strength of Cu-Ni 70 / 30 Threaded Bushing Forged Fittings are improved by the addition of iron, niobium, manganese, and or chromium. The addition of small amounts of iron and manganese make Copper Nickel 70 / 30 Threaded Plug Forged Fittingsideal for use in applications involving high-velocity polluted seawater. Cupro Nickel C71500Threaded Forged Fittingsare currently used in sizeable quantities for power, offshore,and desalination industries.
Copper Nickel 70/30 Threaded Cap, CU-Ni 70/30 Threaded Bend, CU-Ni 70/30 Threaded Weld Cross, UNS C71500 Threaded Bushing, DIN 2.0882 Threaded Coupling, Cupro Nickel 70/30 Threaded Union Suppliers in India.
Key Charactristic:
- Corrosion resistance
- Resistance to oxidation and sulfidation
- Cryogenic strength
- Resistance to abrasion and erosion
- Surface finish
- Magnetic properties
- Ductility
- Elevated temperature strength
- Stability of properties in service
- Suitability for intended fabrication techniques
Copper Nickel 70/30 Threaded Forged Fittings Specifications
| Grade | Copper Nickel 70-30 | UNS C71500 |
| Standard | ASTM B122, ASTM B171, ASTM B466, ASTM B467 |
| Dimensions | ASME 16.11, MSS SP-79, 83, 95, 97, BS 3799 |
| Size | 1/8” NB to 4” NB (Socketweld & Screwed-Threaded) |
| Class | 70-300 LBS, 3000 LBS, 70-300 LBS, 9000 LBS |
| Form | Threaded 45 deg Elbow, Threaded 90 deg Elbow, Threaded Tee, Threaded Cross, Threaded Cap, Threaded Bend, Threaded Coupling, Threaded Union , Threaded Bushing, Plug, Hex Plus, Hexagonal Plus, Lateral Tee. |
| Type | Threaded Forged Fittings |
| Standard | Copper Nickel 70-30 |
| UNS | C71500 |
| WERKSTOFF NR. | 2.0882 |
Copper Nickel 70/30 Threaded Forged Fittings Chemical Composition
| Grade | Cu | Mn | Pb | Ni | Fe | Zn |
| Cupro Nickel 70/30 | 65 min | 1.0 max | 0.05 max | 29-33 max | 0.4-1.0 max | 1 max |
Copper Nickel 70/30 Threaded Forged Fittings Mechanical Properties
| Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
| 0.323 lb/in3 at 68 F | 2260 F | 50000 psi | 20000 psi | 30 % |
Other Types of Copper Nickel 70/30 Threaded Forged Fittings
- Copper Nickel 70/30 Forged Elbow Supplier in UAE
- Cupro Nickel 70/30 Equal Tee Manufacturer in India
- Cu-Ni 70/30 Threaded Cross
- UNS C71500 Threaded Union
- UNS C71500 Hexagonal Plug
- DIN 2.0882 Threaded Hex Plug
- DIN 2.0882 45 Deg Threaded Elbow Distributors
- Cu-Ni 70/30 Threaded Bushing
- Copper Nickel 70/30 Threaded Lateral Tee
- Cupro Nickel 70/30 Alloy Threaded Cross
- Copper Nickel 70/30 Threaded Coupling Exporter in Russia
- Cupro Nickel 70/30 Threaded Tees
- UNS C71500 45 deg Elbow Supplier in Poland
- UNS C71500 Threaded 90 deg Elbow
- DIN 2.0882 Threaded Cap in Qatar
- DIN 2.0882 Threaded Bend Flanges
- Cu-Ni 70/30 Threaded Union
- Cu-Ni 70/30 Threaded Bushing
- Copper Nickel 70/30 Lateral Tee
- Cupro Nickel 70/30 Threaded Cross
Countries We Export to
Nickel Super Alloys manufactures and exports Copper Nickel 70/30 Threaded Forged Fittings to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia
Cities We Deliver to
Nickel Super Alloys manufactures and exports Copper Nickel 70/30 Threaded Forged Fittings to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo