Alloy Steel F22 Threaded Forged Fittings
F22 Chrome Moly Forged Threaded 90 Deg. Elbow, Alloy Steel F22 Threaded Tee, ASME SA182M Alloy Steel F22 Threaded Cross, F22 Chrome Moly Threaded Forged Cap Manufacturer in Mumbai, India.
Nickel Super Alloys is a well-known Manufacturer of Alloy Steel F22 Threaded Forged Fittings, which are supplied by us to various industries. Alloy Steel F22 Threaded Elbow Forged Fittings has features like Excellent performance, Easy installation, Reliable operation, Excellent quality, Smooth texture, High performance, Rust free, Different options, Strongly welded, Corrosion & Abrasion Resistant, Affordable Prices, High Grade Raw Material, and more. Backed by quality fabrication support, these Alloy Steel F22 Threaded Tee Forged Fittings are developed using finest quality stainless steel so as to add to the perfect finish and superior finish quality of the end product. Moreover, clients can avail Alloy Steel F22 Threaded Cross Forged Fittingsat cost effective prices.
The hot - working range for Alloy Steel F22 Threaded Cap Forged Fittingsis 1600 Degree F to 2150 Degree F. These Alloy Steel F22 Threaded Bend Forged Fittings have undergone stringent quality check and have been certified by national authorities. Alloy Steel F22 Threaded Coupling Forged Fittings is often used in Automotive, Industrial Heating, Chemical Processing, Nuclear power generation, Medical Devices, Oil & Gas, etc. Alloy Steel F22 Threaded Union Forged Fittings offers improved weldability and also reduces the possibility of lower corrosion resistance around welded areas. Being a quality based firm, we are engaged in offering a quality assured assortment of Alloy Steel F22 Threaded Bushing Forged Fittings, which is widely demanded for its sturdiness and supreme quality.
ASTM A182 Alloy Steel F22 Threaded Cap, ASME 16.11 Alloy Steel F22 Threaded Bend, Alloy Steel F22 Threaded Weld Cross, Alloy Steel F22 Threaded Bushing, F22 Alloy Steel Threaded Coupling, Alloy Steel F22 Threaded Union Suppliers in India.
Key Charactristic:
- Corrosion resistance
- Resistance to oxidation and sulfidation
- Cryogenic strength
- Resistance to abrasion and erosion
- Surface finish
- Magnetic properties
- Ductility
- Elevated temperature strength
- Stability of properties in service
- Suitability for intended fabrication techniques
Alloy Steel F22 Threaded Forged Fittings Specifications
| Grade | Alloy Steel Grade F22 |
| Standard | ASTM A182, ASME SA182 |
| Dimensions | ASME 16.11, MSS SP-79, 83, 95, 97, BS 3799 |
| Size | 1/8” NB to 4” NB (Socketweld & Screwed-Threaded) |
| Class | F220 LBS, 3000 LBS, F220 LBS, 9000 LBS |
| Form | Threaded 45 deg Elbow, Threaded 90 deg Elbow, Threaded Tee, Threaded Cross, Threaded Cap, Threaded Bend, Threaded Coupling, Threaded Union , Threaded Bushing, Plug, Hex Plus, Hexagonal Plus, Lateral Tee. |
| Type | Threaded Forged Fittings |
Alloy Steel F22 Threaded Forged Fittings Chemical Composition
| Grade | C | Mn | Si | S | P | Cr | Mo |
| Alloy Steel F22 | 0.05-0.15 | 0.3-0.6 | 0.5 | 0.03 | 0.045 | 0.8-1.25 | 0.44-0.65 |
Alloy Steel F22 Threaded Forged Fittings Mechanical Properties
| Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
| 205 | 415 | 20 % |
Other Types of Alloy Steel F22 Threaded Forged Fittings
- Alloy Steel F22 Forged Elbow Supplier in UAE
- Gr F22 Alloy Equal Tee Manufacturer in India
- Alloy Steel F22 Threaded Cross
- Alloy Steel F22 Threaded Union
- F22 Chrome Moly Hexagonal Plug
- F22 Chrome Moly Threaded Hex Plug
- Alloy Steel F22 45 Deg Threaded Elbow Distributors
- Alloy Steel F22 Threaded Bushing
- Grade F22 Alloy Threaded Lateral Tee
- Grade F22 Alloy Threaded Cross
- Alloy Steel F22 Threaded Coupling Exporter in Russia
- Alloy Steel F22 Threaded Tees
- Gr F22 Alloy Threaded 45 deg Elbow Supplier in Poland
- Gr F22 Alloy Threaded 90 deg Elbow
- F22 Chrome Moly Threaded Cap in Qatar
- F22 Chrome Moly Threaded Bend Flanges
- Alloy Steel F22 Threaded Union
- Alloy Steel F22 Threaded Bushing
- Alloy Steel F22 Lateral Tee
- Alloy Steel F22 Threaded Cross
Countries We Export to
Nickel Super Alloys manufactures and exports Alloy Steel F22 Threaded Forged Fittings to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia
Cities We Deliver to
Nickel Super Alloys manufactures and exports Alloy Steel F22 Threaded Forged Fittings to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo