Stainless Steel 316 / 316L / 316Ti Threaded Forged Fittings
Stainless Steel 316 / 316L Socket Weld 90 Deg. Elbow, UNS S31600 / S31008 / S31635 Socket Weld Tee, DIN NR. 1.4401/1.4436 Socket Weld Cross, SS 316 Socket Weld Forged Cap Manufacturer in Mumbai, India.
Nickel Super Alloys is one of the leading distributor and supplier of Stainless Steel 316 / 316L / 316Ti Socket Weld Forged Fittings, which guarantee an excellent corrosion resistance. Stainless Steel 316 Socket Weld Elbow Forged Fittings is often utilized in process streams containing chlorides or halides. The addition of molybdenum in Stainless Steel 316 Socket Weld Tee Forged Fittings improves general corrosion and chloride pitting resistance. Stainless Steel 316 Socket Weld Cross Forged Fittings also offer stress-rupture, tensile strength and higher creep at elevated temperature. Stainless Steel 316 Socket Weld Cap Forged Fittings has better corrosion resistance at higher temperatures. Stainless Steel 316 Socket Weld Coupling Forged Fittings can be susceptible to sensitization, which will reduce the formation of chromium carbides.
The use of a higher alloyed filler metal like Stainless Steel 316 Socket Weld Union Forged Fittings can be necessary due to the cast structure of the weld metal. Stainless Steel 316 Socket Weld Plug Forged Fittings has the addition of molybdenum in its composition, which provides increased strength at elevated temperatures.Stainless Steel 316 Socket Weld Bushing Forged Fittings isparticularly apparent for pitting and crevice corrosion in chloride environments. Additionally, Stainless Steel UNS S31600 Socket Weld Forged Fittings are weldable and formable, which drastically enhances corrosion resistance. Stainless Steel UNS S31603 Socket Weld Forged Fittings is often used in the architectural, industrial, and transportation fields. Stainless Steel UNS S31609 Socket Weld Forged Fittings exhibit better corrosion resistance.
Stainless Steel 316L Socket Weld Cap, Stainless Steel 316 Socket Weld Bend, SS 316L Socket Weld Cross, UNS S31600 / S31008 / S31635 Socket Weld Bushing, DIN NR. 1.4404/1.4435 Socket Weld Coupling, Stainless Steel 316 Socket Weld Union Suppliers in India.
Key Charactristic:
- Corrosion resistance
- Resistance to oxidation and sulfidation
- Cryogenic strength
- Resistance to abrasion and erosion
- Surface finish
- Magnetic properties
- Ductility
- Elevated temperature strength
- Stability of properties in service
- Suitability for intended fabrication techniques
Stainless Steel 316 / 316L / 316Ti Socket Weld Forged Fittings Specifications
| Grade | SS 316 | SS 316L , UNS S31600 | S31608 |
| Standard | ASTM A182 & ASME SA182 |
| Dimensions | ASME 16.11, MSS SP-79, 83, 95, 97, BS 3799 |
| Size | 1/8” NB to 4” NB (Socketweld & Screwed-Threaded) |
| Class | 2000 LBS, 3000 LBS, 6000 LBS, 9000 LBS |
| Form | Socket Weld Elbow, Socket Weld Tee, Socket Weld Cross, Socket Weld Cap, Socket Weld Coupling, Socket Weld Union , Socket Weld Plug, Socket Weld Lateral Tee. |
| Type | Socket Weld Fittings |
| STANDARD | WERKSTOFF NR. | UNS | JIS | BS | GOST | AFNOR | EN |
| SS 316 | 1.4401/1.4436 | S31600 | SUS 316 | 316S31 / 316S33 | – | Z7CND17‐11‐02 | X5CrNiMo17-12-2 / X3CrNiMo17-13-3 |
| SS 316L | 1.4404/1.4435 | S31008 | SUS 316L | 316S11 / 316S13 | 03Ch17N14M3 / 03Ch17N14M2 | Z3CND17‐11‐02 / Z3CND18‐14‐03 | X2CrNiMo17-12-2 / X2CrNiMo18-14-3 |
| SS 316Ti | 1.4571 | S31635 | SUS 316Ti | 320S31 | 08Ch17N13M2T | Z6CNDT17‐123 | X6CrNiMoTi17-12-2 |
Stainless Steel 316 / 316L / 316Ti Socket Weld Forged Fittings Chemical Composition
| Grade | C | Mn | Si | P | S | Cr | Mo | Ni | N |
| SS 316 | 0.008max | 2 max | 1.00 max | 0.045 max | 0.030 max | 16 – 18 | 2.00-3.00 | 11.00-14.00 | – |
| SS 316L | 0.035 max | 2 max | 1.00 max | 0.045 max | 0.030 max | 16– 18 | 2.00-3.00 | 10.00 – 14.00 | – |
| SS 316Ti | 0.08 max | 2 max | 0.75 max | 0.045 max | 0.030 max | 16 – 18 | 2.00-3.00 | 10.00 – 14.00 | 68.395 min |
Stainless Steel 316 / 316L / 316Ti Socket Weld Forged Fittings Mechanical Properties
| Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
| 8.0 g/cm3 | 1400 °C (2550 °F) | Psi – 75000 , MPa – 515 | Psi – 30000 , MPa – 205 | 35 % |
Other Types of Stainless Steel 316 / 316L / 316Ti Socket Weld Threaded Forged Fittings
- Stainless Steel 316 Socket Weld Forged Elbow Supplier in UAE
- SS 316L Socket Weld Equal Tee Manufacturer in India
- SS 316 Socket Weld Cross
- UNS S31600 / S31008 / S31635 Socket Weld Union
- UNS S31600 / S31008 / S31635 Socket Weld Plug
- DIN NR. 1.4401 / 1.4436 Socket Weld Hex Plug
- DIN NR. 1.4404 / 1.4435 45 Deg Socket Weld Elbow Distributors
- Stainless Steel 316 Socket Weld Bushing
- Stainless Steel 316L Socket Weld Lateral Tee
- SUS 316 Socket Weld Cross
- Stainless Steel 316 Socket Weld Coupling Exporter in Russia
- Stainless Steel 316L Socket Weld Tees
- UNS S31600 / S31008 / S31635 45 deg Socket Weld Elbow Supplier in Poland
- UNS S31600 / S31008 / S31635 Socket Weld 90 deg Elbow
- DIN NR. 1.4571 Socket Weld Cap in Qatar
- DIN NR. 1.4404 / 1.4435 Socket Weld Bend Flanges
- SS 316L Socket Weld Union
- X5CrNiMo17-12-2 / X3CrNiMo17-13-3 Socket Weld Bushing
- X2CrNiMo17-12-2 / X2CrNiMo18-14-3 Socket Weld Lateral Tee
- X6CrNiMoTi17-12-2 Socket Weld Cross
Countries We Export to
Nickel Super Alloys manufactures and exports Stainless Steel 316 / 316L / 316Ti Socket Weld Forged Fittings to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia
Cities We Deliver to
Nickel Super Alloys manufactures and exports Stainless Steel 316 / 316L / 316Ti Socket Weld Forged Fittings to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo