Incoloy 925 Flanges
Alloy 925 Spacer Ring Flanges, Incoloy 925 Nipo Flange, Incoloy Alloy 925 Orifice Flanges, UNS N09925 Incoloy SORF Flange, Incoloy 925 Threaded Flanges, Manufacturer in Mumbai,India.
Nickel Super Alloys is one of the leading names in manufacturing Inconel Alloy 925 Flanges, which is a precipitation-hardenable nickel-iron-chromium alloy. Inconel 925 Slip On Raised Flanges is known for a number of different unique characteristics including such as protection in oxidizing and reducing atmosphere. We make a comprehensive range of Inconel 925 Blind Raised Flanges in most standard wrought forms. In combination with molybdenum and copper, Inconel 925 Spectacle Blind Flanges gives outstanding resistance to reducing chemicals. Inconel 925 Threaded Flanges is used in various applications requiring a combination of high strength and corrosion resistance.
Chromium in Inconel 925 Weld Neck Flanges is the hardest metal element and the only element that exhibits antiferromagnetic ordering at room temperature, above which it transforms into a paramagnetic solid. Thechromium content in Inconel 925 Socket Weld Flanges provides resistance to oxidizing environments. Forging in Inconel 925 Lap Joint Flangesshould be done in the range of 2150 Degree F to 1700 Degree F. Pitting and crevice corrosion resistance in Inconel 925 Ring Joint Type Flanges is also excellent. Molybdenum in Inconel 925 Spacer Flanges enhances resistance to pitting and crevice corrosion, lifting the Pitting Resistance Equivalent. During heat treatment, a strengthening reaction in Inconel 925 Long Weld Neck Flanges is caused by the addition of titanium and aluminum. We offer non heat treatment or heat treatment for Inconel 925 Nippolet Flanges (normalizing,annealing, and high temperature tempering) state of delivery.
ASME B16.5 Alloy 925 WNRF Flanges, Incoloy 925 Lap Joint Flanges, Alloy 925 Ring Type Joint Flanges, Incoloy Alloy 925 Spectacle Blind Flanges, UNS N09925 Alloy Forged Flanges, ANSI B16.47 Plate Flanges Suppliers in India.
Key Charactristic:
- Corrosion resistance
- Resistance to oxidation and sulfidation
- Cryogenic strength
- Resistance to abrasion and erosion
- Surface finish
- Magnetic properties
- Ductility
- Elevated temperature strength
- Stability of properties in service
- Suitability for intended fabrication techniques
Incoloy 925 Flanges Specifications
| Grade | Incoloy Alloy 925 / UNS N09925 |
| Standard | ASTM B564, ASME SB564 |
| Dimensions | ANSI / ASME B16.5, B16.47 Series A & B, B.16.48, BS4504, BS10, DIN, EN-1092, MSS SP44 |
| Size | 1/2" - 48" (15NB - 1200NB) |
| Class / Pressure Rating | 150 Class, 300 Class, 925 Class, 900 Class, 1500 Class, 2500 Class, PN6, PN10, PN16, PN25, PN40, PN64, etc. |
| Form | Slip on Flanges (SORF), Threaded Flanges, Weld neck Flanges (WNRF), Blind Flanges, Socket weld Flanges, Lap Joint Flanges, Ring Type Joint Flanges, Spectacle Blind Flanges, Spacer Ring Flanges, Long weld Neck Flanges, Nipo Flange, Nipolet Flanges, Plate Flanges, Flat Flange, Orifice Flanges, Forged Flanges |
| Flange Face Type | Flat Face (FF), Raised Face (RF), Ring Type Joint(RTJ) |
| Standard | Incoloy 925 |
| UNS | N09925 |
| WERKSTOFF NR. | - |
Incoloy 925 Flanges Chemical Composition
| Grade | Ni | Cr | Fe | Si | Mo | Cu | Mn | C | S | Al |
| Incoloy 925 | 42 – 46 | 19.55 – 22.5 | 22 min | 0.5 max | 2.5 – 3.5 | 1.5 – 3.0 | 1.0 max | 0.03 max | 0.03 max | 0.1 – 0.5 |
Incoloy 925 Flanges Mechanical Properties
| Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
| 8.14 g/cm3 | 1343°C | 650 | 300 | 30 % |
Other Types of Incoloy 925 Flanges
- Incoloy 925 Tongue & Groove Flanges Supplier in UAE
- Incoloy 925 Spectacle blind flanges Manufacturer in India
- Inconel 925 Long Weld Neck Flanges
- Incoloy 925 Flat Face Flanges
- UNS N09925 High Hub Blind Flanges
- UNS N09925 Lap Joint Flanges
- N09925 Reducing Flanges Distributors
- N09925 Blind Flanges
- Incoloy 925 Slip On Flanges
- UNS N09925 Threaded Flanges
- Incoloy 925 Orifice Flanges Exporter in Russia
- Incoloy 925 400# Forged Flanges
- Incoloy 925 F91 600# Plate Flanges Supplier in Poland
- Incoloy 925 900# Spacer Ring Flanges
- N09925 PN6 Nipo Flange in Qatar
- N09925 PN10 Nipolet Flanges
- Incoloy 925 Pipe Flanges
- Incoloy 925 SORF Flanges
- Incoloy 925 WNRF Flanges
- Incoloy 825 Threaded Flanges
Countries We Export to
Nickel Super Alloys manufactures and exports Incoloy 925 Flanges to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia
Cities We Deliver to
Nickel Super Alloys manufactures and exports Incoloy 925 Flanges to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo