Incoloy 825 Flanges
ASTM B564 Incoloy 825 RTJ Flange, ANSI B16.5 Alloy 825 Orifice Flange, Incoloy 825 Threaded Flanges, ASME SB564 Alloy 825 Lap Joint Flange, Inconel 825 Spectacle Blind Flanges, Manufacturer in Mumbai,India.
Nickel Super Alloys is one of the leading supplier and distributor of Inconel Alloy 825 Flanges, which is a nickel-chromium alloy with additions of molybdenum and copper. Inconel 825 Slip On Raised Flanges is designed for use in extremely corrosive environments. Inconel 825 Blind Raised Flanges has practical immunity to chloride stress corrosion cracking (SCC). The chromium content in Inconel 825 Spectacle Blind Flanges confers resistance to a variety of oxidizing substances such as nitrates, oxidising salt and nitric acid. Inconel 825 Threaded Flanges are mainly used in the harshest chemical environments of all, involving among others, acids, wet scrubbing, etc.Inconel 825 Socket Weld Flangesi s especially resistant to sulfuric and phosphoric acids.
The titanium addition serves, with an appropriate heat treatment, to stabilize Inconel 825 Weld Neck Flanges against sensitization to inter-granular corrosion. Inconel 825 Spacer Flanges is titanium stabilised to resist pitting and intergranular attack after fabrication, particularly welding. The addition of titanium stabilizes Inconel 825 Lap Joint Flanges against sensitization in the as-welded condition. These Inconel 825 Ring Joint Type Flanges are sourced from our reliable experts who manufacture them from high grade material. Inconel 825 Long Weld Neck Flanges is supplied in the hot worked and annealed condition. Inconel UNS N08825 Flanges has low strength and excellent corrosion resistance in a range of media. Inconel WNR 2.4858 Flanges possesses extremely high corrosion resistance against oxidizing and non-oxidizing acids.
Incoloy 825 Blind Flanges, Incoloy 825 Pipe Flanges, Incoloy UNS N08825 Pipe Flanges, Inconel 825 Nippolet Flanges, Incoloy 825 Slip On Flanges, Inconel 825 Long weld neck Flnges, DIN 2.4858 Socket Weld Flanges Suppliers in India.
Key Charactristic:
- Corrosion resistance
- Resistance to oxidation and sulfidation
- Cryogenic strength
- Resistance to abrasion and erosion
- Surface finish
- Magnetic properties
- Ductility
- Elevated temperature strength
- Stability of properties in service
- Suitability for intended fabrication techniques
Incoloy 825 Flanges Specifications
| Grade | Incoloy Alloy 825 / UNS N08825 |
| Standard | ASTM B564, ASME SB564 |
| Dimensions | ANSI / ASME B16.5, B16.47 Series A & B, B.16.48, BS4504, BS10, DIN, EN-1092, MSS SP44 |
| Size | 1/2" - 48" (15NB - 1200NB) |
| Class / Pressure Rating | 150 Class, 300 Class, 825 Class, 900 Class, 1500 Class, 2500 Class, PN6, PN10, PN16, PN25, PN40, PN64, etc. |
| Form | Slip on Flanges (SORF), Threaded Flanges, Weld neck Flanges (WNRF), Blind Flanges, Socket weld Flanges, Lap Joint Flanges, Ring Type Joint Flanges, Spectacle Blind Flanges, Spacer Ring Flanges, Long weld Neck Flanges, Nipo Flange, Nipolet Flanges, Plate Flanges, Flat Flange, Orifice Flanges, Forged Flanges |
| Flange Face Type | Flat Face (FF), Raised Face (RF), Ring Type Joint(RTJ) |
| Standard | Incoloy 825 |
| UNS | N08825 |
| GOST | ЭП703 |
| AFNOR | NFE30C20DUM |
| BS | NA 16 |
| JIS | NCF 825 |
| EN | NiCr21Mo |
| WERKSTOFF NR. | 2.4858 |
| OR | XH38BT |
Incoloy 825 Flanges Chemical Composition
| Grade | C | Mn | Si | S | Cu | Fe | Ni | Cr | Al | Ti |
| 825 | 0.05 max | 1.00 max | 0.5 max | 0.03 max | 1.50 – 3.00 | 22.00 min | 38.00 – 46.00 | 19.50 – 23.50 | 0.02 max | 0.06 – 1.20 |
Incoloy 825 Flanges Mechanical Properties
| Element | Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
| 825 | 8.14 g/cm3 | 1400 °C (2550 °F) | Psi – 80,000 , MPa – 550 | Psi – 32,000 , MPa – 220 | 30 % |
Other Types of Incoloy 825 Flanges
- Incoloy 825 Tongue & Groove Flanges Supplier in UAE
- Incoloy 825 Spectacle blind flanges Manufacturer in India
- Inconel 825 Long Weld Neck Flanges
- Incoloy 825 Flat Face Flanges
- UNS N08825 High Hub Blind Flanges
- UNS N08825 Lap Joint Flanges
- DIN 2.4858 Reducing Flanges Distributors
- DIN 2.4858 Blind Flanges
- Incoloy 825 Slip On Flanges
- UNS N08825 Threaded Flanges
- Incoloy 825 Orifice Flanges Exporter in Russia
- Incoloy 825 400# Forged Flanges
- Incoloy 825 F91 600# Plate Flanges Supplier in Poland
- Incoloy 825 900# Spacer Ring Flanges
- DIN 2.4858 PN6 Nipo Flange in Qatar
- DIN 2.4858 PN10 Nipolet Flanges
- UNS N08825 Pipe Flanges
- UNS N08825 SORF Flanges
- Incoloy 825 WNRF Flanges
- Incoloy 825 Threaded Flanges
Countries We Export to
Nickel Super Alloys manufactures and exports Incoloy 825 Flanges to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia
Cities We Deliver to
Nickel Super Alloys manufactures and exports Incoloy 825 Flanges to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo