Hastelloy X Flanges
Hastelloy X Slip On Flanges, Hastelloy X Nippolet Flangs, X Hastelloy WNRF Flanges, Alloy X Blind Flanges, Hastelloy X Weld Neck Flange, UNS N06002 RTJ Flange, DIN 2.4665 Lap Joint Flange Manufacturer in Mumbai,India.
Nickel Super Alloys is a known supplier and manufacturer of Hastelloy Alloy X Flanges, which has excellent forming and welding characteristics. Hastelloy X Slip On Raised Flangesis easily fabricated including forming and welding. Hastelloy X Blind Raised Flanges offers excellent corrosion resistance properties similar to high nickel alloys more commonly in corrosion applications. Hastelloy X Spectacle Blind Flanges are provided in the solution heat-treated condition. Hastelloy X Threaded Flanges is normally supplied in the solution-treated condition, following a treatment at 1175 Degree C and rapid cooling.Hastelloy X Weld Neck Flangesis especially resistant to carburization and nitriding, conditions which cause failure in some high temperature alloys. As a consequence of its good ductility, Hastelloy X Socket Weld Flanges is also readily formed by cold-working. Hastelloy X Lap Joint Flanges retains oxidation resistance at high temperatures.
Wrought forms of Hastelloy X Ring Joint Type Flanges are furnished in thesolution heat-treated conditionunless otherwise specified. Hastelloy X Spacer Flanges resistsin two common conditions that often lead to early failure in high temperature alloys, carburization and nitriding. Hastelloy X Long Weld Neck Flanges has no yield or tensile strength requirements. Hastelloy X Long Weld Neck Flanges has many different industrial component applications, some of which include combustion chambers. Hastelloy X Nippolet Flangesi s being able to withstand reducing or neutral atmospheres and oxidation. Hastelloy UNS N06002 Flanges has good ductility after prolonged exposure at high-temperatures.
ASME SB564 Hastelloy X Threaded Flanges, Hastelloy X Socket Weld Flanges, Hastelloy X Flanges, ANSI B16.5 Hastelloy X Ring Type Joint Flanges, 150# ANSI Alloy X Flanges, UNS N06002 Pipe Flanges Suppliers in India.
Key Charactristic:
- Corrosion resistance
- Resistance to oxidation and sulfidation
- Cryogenic strength
- Resistance to abrasion and erosion
- Surface finish
- Magnetic properties
- Ductility
- Elevated temperature strength
- Stability of properties in service
- Suitability for intended fabrication techniques
Hastelloy X Flanges Specifications
| Grade | Hastelloy Alloy X / UNS N06002 |
| Standard | ASTM B564, ASME SB564 |
| Dimensions | ANSI / ASME B16.5, B16.47 Series A & B, B.16.48, BS4504, BS10, DIN, EN-1092, MSS SP44 |
| Size | 1/2" - 48" (15NB - 1200NB) |
| Class / Pressure Rating | 150 Class, 300 Class, X Class, 900 Class, 1500 Class, 2500 Class, PN6, PN10, PN16, PN25, PN40, PN64, etc. |
| Form | Slip on Flanges (SORF), Threaded Flanges, Weld neck Flanges (WNRF), Blind Flanges, Socket weld Flanges, Lap Joint Flanges, Ring Type Joint Flanges, Spectacle Blind Flanges, Spacer Ring Flanges, Long weld Neck Flanges, Nipo Flange, Nipolet Flanges, Plate Flanges, Flat Flange, Orifice Flanges, Forged Flanges |
| Flange Face Type | Flat Face (FF), Raised Face (RF), Ring Type Joint(RTJ) |
| Standard | Hastelloy X |
| UNS | N06002 |
| WERKSTOFF NR. | - |
Hastelloy X Flanges Chemical Composition
| Grade | Ni | Mo | Cr | Fe | Mn | C | Co | Si | P | S |
| Hastelloy X | Balance | 8.00 – 10.00 | 20.50 – 23.00 | 17.00 – 20.00 | 1.00 max | 0.05 – 0.15 | 0.50 – 2.50 | 1.00 max | 0.04 max | 0.03 max |
Hastelloy X Flanges Mechanical Properties
| Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
| 8.22 g/cm³ | 1355°C | 655 MPa | 240 MPa | 35% |
Other Types of Hastelloy X Flanges
- Hastelloy X Tongue & Groove Flanges Supplier in UAE
- Hastelloy X Spectacle blind flanges Manufacturer in India
- Hastelloy X Long Weld Neck Flanges
- Hastelloy X Flat Face Flanges
- UNS N06002 High Hub Blind Flanges
- UNS N06002 Lap Joint Flanges
- DIN 2.4665 Reducing Flanges Distributors
- DIN 2.4665 Blind Flanges
- Hastelloy X Slip On Flanges
- UNS N06002 Threaded Flanges
- Hastelloy X Orifice Flanges Exporter in Russia
- Hastelloy X 400# Forged Flanges
- Hastelloy X F91 600# Plate Flanges Supplier in Poland
- Hastelloy X 900# Spacer Ring Flanges
- DIN 2.4665 PN6 Nipo Flange in Qatar
- DIN 2.4665 PN10 Nipolet Flanges
- Hastelloy X Pipe Flanges
- UNS N06002 SORF Flanges
- Hastelloy X WNRF Flanges
- Hastelloy X Threaded Flanges
Countries We Export to
Nickel Super Alloys manufactures and exports Hastelloy X Flanges to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia
Cities We Deliver to
Nickel Super Alloys manufactures and exports Hastelloy X Flanges to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo