Hastelloy C276 Flanges
Hastelloy UNS N10276 Pipe Flanges, ANSI B16.5 Alloy C276 Ring Type Joint Flanges, Alloy C276 Blind Flanges Stockholder, Hastelloy C276 Spacer, Hastelloy C276 Screwed Flanges Manufacturer in Mumbai,India.
Nickel Super Alloys is a known supplier and exporter of Hastelloy Alloy C276 Pipe Flanges, which have good oxidation and creep resistance. Hastelloy C276 Slip On Raised Flanges offers exceptional resistance to strong solutions of oxidizing salts such as cupric andferric chlorides. Hastelloy C276 Blind Raised Flanges is resistant to the formation of grain boundary precipitates in the weld heat-affected zone. Hastelloy C276 Spectacle Blind Flanges is very resistant to sulfide stress cracking and SCC in sour, oilfield environments. Hastelloy C276 Threaded Flanges is not prone to grain boundary precipitation in the as welded condition. Hastelloy C276 Socket Weld Flanges is used in a variety of environments from moderately oxidizing to strong reducing conditions.
Hastelloy C276 Weld Neck Flanges has excellent resistance to phosphoric acid at all temperatures below boiling and concentrations. More so than any other Ni-Cr-Mo alloy, Hastelloy C276 Ring Joint Type Flanges metal has become the steel of choice for corrosion resistance and versatility. Hastelloy C276 Lap Joint Flanges resists many of the most severe media encountered in chemical processing, including reducing and oxidizing acids. Hastelloy C276 Spacer Flanges also has excellent resistance to corrosion by seawater especially under crevice conditions which induce attack in other commonly used materials. Hastelloy C276 Long Weld Neck Flanges cannot be hardened by heat treatment, but can be hardened by cold working. Hastelloy C276 Nippolet Flanges is readily fabricated by welding, using methods similar to those utilized for nickel-based alloys.
ASME SB564 Alloy C276 Lap Joint Flange, Hastelloy C276 Spectacle Blind Flanges, Hastelloy DIN 2.4819 Socket Weld Flanges, Hastelloy C276 Nippolet Flanges, Hastelloy C276 Pipe Flanges, Hastelloy C276 Slip On Flanges, Suppliers in India.
Key Charactristic:
- Corrosion resistance
- Resistance to oxidation and sulfidation
- Cryogenic strength
- Resistance to abrasion and erosion
- Surface finish
- Magnetic properties
- Ductility
- Elevated temperature strength
- Stability of properties in service
- Suitability for intended fabrication techniques
Hastelloy C276 Flanges Specifications
| Grade | Hastelloy Alloy C276 / UNS N10276 |
| Standard | ASTM B564, ASME SB564 |
| Dimensions | ANSI / ASME B16.5, B16.47 Series A & B, B.16.48, BS4504, BS10, DIN, EN-1092, MSS SP44 |
| Size | 1/2" - 48" (15NB - 1200NB) |
| Class / Pressure Rating | 150 Class, 300 Class, C276 Class, 900 Class, 1500 Class, 2500 Class, PN6, PN10, PN16, PN25, PN40, PN64, etc. |
| Form | Slip on Flanges (SORF), Threaded Flanges, Weld neck Flanges (WNRF), Blind Flanges, Socket weld Flanges, Lap Joint Flanges, Ring Type Joint Flanges, Spectacle Blind Flanges, Spacer Ring Flanges, Long weld Neck Flanges, Nipo Flange, Nipolet Flanges, Plate Flanges, Flat Flange, Orifice Flanges, Forged Flanges |
| Flange Face Type | Flat Face (FF), Raised Face (RF), Ring Type Joint(RTJ) |
| Standard | Hastelloy C276 |
| EN | NiMo16Cr15W |
| UNS | N10276 |
| OR | ЭП760 |
| JIS | NW 0276 |
| GOST | ХН65МВУ |
| AFNOR | NFE30C20DUM |
| WERKSTOFF NR. | 2.4819 |
| BS | - |
Hastelloy C276 Flanges Chemical Composition
| Grade | C | Mn | Si | S | Co | Ni | Cr | Fe | Mo | P |
| C276 | 0.010 max | 1.00 max | 0.08 max | 0.03 max | 2.50 max | 50.99 min* | 14.50 – 16.50 | 4.00 – 7.00 | 15.00 – 17.00 | 0.04 max |
Hastelloy C276 Flanges Mechanical Properties
| Element | Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
| Hastelloy C276 | 8.89 g/cm3 | 1370 °C (2500 °F) | Psi – 1,15,000 , MPa – 790 | Psi – 52,000 , MPa – 355 | 40 % |
Other Types of Hastelloy C276 Flanges
- Hastelloy C276 Tongue & Groove Flanges Supplier in UAE
- Hastelloy C276 Spectacle blind flanges Manufacturer in India
- Hastelloy C276 Long Weld Neck Flanges
- Hastelloy C276 Flat Face Flanges
- UNS N10276 High Hub Blind Flanges
- UNS N10276 Lap Joint Flanges
- DIN 2.4819 Reducing Flanges Distributors
- DIN 2.4819 Blind Flanges
- Hastelloy C276 Slip On Flanges
- UNS N10276 Threaded Flanges
- Hastelloy C276 Orifice Flanges Exporter in Russia
- Hastelloy C276 400# Forged Flanges
- Hastelloy C276 F91 600# Plate Flanges Supplier in Poland
- Hastelloy C276 900# Spacer Ring Flanges
- DIN 2.4819 PN6 Nipo Flange in Qatar
- DIN 2.4819 PN10 Nipolet Flanges
- Hastelloy C276 Pipe Flanges
- UNS N10276 SORF Flanges
- Hastelloy C276 WNRF Flanges
- Hastelloy C276 Threaded Flanges
Countries We Export to
Nickel Super Alloys manufactures and exports Hastelloy C276 Flanges to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia
Cities We Deliver to
Nickel Super Alloys manufactures and exports Hastelloy C276 Flanges to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo