Tube End Closure Tube Fittings
Stainless Steel Tube End Closure Tube Fittings, Alloy Steel Tube End Closure Tube Fittings, Carbon Steel Tube End Closure Tube Fittings, Nickel Alloy Tube End Closure Pipe Fittings Manufacturer in Mumbai,India.
Nickel Super Alloys is one of leading supplier and distributor of Tube End Closure in India. Tube End Closure has a unique three-piece design having a body, with as hardened ferrule and nut. Unlike traditional compression joint, this nut is screwed on to the body. This ferrule grips the pipe in position and perceptibly holds the pipe surface to provide a positive seal. When it is fully tightened ferrule is distorted slightly in the middle sections and acts as a spring. Our offered range of Tube End Closure Fittings is available in Brass, Stainless Steel, Alloy Steel, Carbon Steel, Nickel Alloy, Monel, Hastelloy, Inconel, Alloy 20, and many other materials. If you don't see the exact product you're looking for, please call us for a quote.
Hastelloy Tube End Closure Fittings, Monel Tube End Closure Tube Fittings, Aluminum Tube End Closure Tube Fittings, Inconel Tube End Closure Fittings Supplier in India
Tube End Closure INCH OD Tubes
| T Tube OD | A | C | D | F A/F |
G A/F |
H |
| 1/16 | 13.0 | 11.0 | 8.6 | 11 | 8 | 11.2 |
| 1/8 | 20.0 | 15.3 | 12.7 | 11 | 11 | 13.5 |
| 1/4 | 23.4 | 17.8 | 15.3 | 14 | 14 | 16.0 |
| 5/16 | 24.4 | 18.5 | 16.3 | 16 | 16 | 17.0 |
| 3/8 | 25.7 | 19.3 | 16.8 | 17 | 17 | 18.3 |
| 1/2 | 29.2 | 21.8 | 22.9 | 22 | 22 | 19.0 |
| 5/8 | 30.0 | 21.8 | 24.4 | 24 | 25 | 19.8 |
| 3/4 | 31.5 | 21.8 | 24.4 | 27 | 28.5 | 21.4 |
| 7/8 | 34 | 21.8 | 25.9 | 35 | 32 | 23.9 |
| 1 | 38.4 | 26.4 | 31.2 | 35 | 38 | 26.2 |
| 1.1/4 | 53.3 | 38.9 | 41.2 | 46 | 50 | 31.2 |
| 1.1/2 | 64.5 | 45.2 | 50.0 | 55 | 57 | 37.4 |
| 2 | 88.6 | 62.7 | 67.6 | 70.0 | 76.0 | 49.3 |
Tube End Closure METRIC OD Tubes
| T Tube OD | A | C | D | F A/F |
G A/F |
H |
| 3 | 20.1 | 15.3 | 12.9 | 11 | 11 | 13.5 |
| 6 | 23.1 | 17.7 | 15.3 | 14 | 14 | 15.7 |
| 8 | 24.5 | 18.6 | 16.2 | 16 | 16 | 17.0 |
| 10 | 26.6 | 19.5 | 17.2 | 17 | 19 | 19.0 |
| 12 | 29.1 | 22.0 | 22.8 | 22 | 22 | 19.0 |
| 14 | 29.9 | 22.0 | 24.4 | 24 | 25 | 19.8 |
| 15 | 29.9 | 22.0 | 24.4 | 24 | 25 | 19.8 |
| 16 | 29.9 | 22.0 | 24.4 | 24 | 25 | 19.8 |
| 18 | 31.4 | 22.0 | 24.4 | 27 | 30 | 21.3 |
| 20 | 34.0 | 22.0 | 26.0 | 32 | 32 | 23.9 |
| 22 | 34.0 | 22.0 | 26.0 | 32 | 32 | 23.9 |
| 25 | 38.5 | 26.5 | 31.3 | 35 | 38 | 26.2 |
| 28 | 48.5 | 36.6 | 36.6 | 41 | 46 | 27.7 |
| 30 | 53.4 | 39.2 | 39.6 | 46 | 50 | 31.8 |
| 32 | 55.8 | 41.6 | 42.0 | 46 | 50 | 32.8 |
| 38 | 65.4 | 47.9 | 49.4 | 55 | 57 | 37.8 |
Material of Construction
| Stainless Steel | ASME / ASTM SA / A403 SA / A 774 WP-S, WP-W, WP-WX, 304, 304L, 316, 316L, 304/304L, 304H, 316H, 316/316L, 321, 330, 347, 309/S, 310/S, 317/L, 333, 410/S, DIN 1.4301, DIN1.4306, DIN 1.4401, DIN 1.4404 |
| Alloy Steel | ASTM SA 182 - E25, E26, E27, E28, E29B, E30B, E39B, E40B, E36B, E36C, E41B, AISI4130, AISI4140, AISI4340, 42CRMO4, 16MNCR5, 20MNCR5, 21CrMoV57, EN353, EN354, F11, F22, F91, F9, P11, P22, P91, P9, P5, P92, EN42J, EN8, EN19 |
| Carbon Steel | ASTM A 234 WPB , WPBW, WPHY 42, WPHY 46, WPHY 52, WPH 60, WPHY 65 & WPHY 70 |
| Monel | Monel 400, Monel K500, Monel R-405 |
| Nickel Alloy | Nickel 200, Nickel 201 |
| Inconel | Inconel 600, Inconel 601, Inconel 625, Inconel 718 |
| Incoloy | Incoloy 800, Inconel 800H, 800HT |
| Hastalloy | Hastalloy B2, Hastalloy B3, Hastalloy C22, Hastalloy C276, Hastalloy X |
| Titanium | Gr1, Gr2, Gr3, Gr5, Gr7, Gr11 |
| Duplex Steel | ASTM / ASME A/SA 182 UNS F44, F45, F51, F53, F55, F60, F61 |
Countries We Export to
Nickel Super Alloys manufactures and exports Tube End Closure to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia
Cities We Deliver to
Nickel Super Alloys manufactures and exports Tube End Closure to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo