45 Degree Threaded Elbow
ASTM A182 Stainless Steel 300 Series 45 Deg Threaded Elbow, SS 45 Deg Threaded Elbow, A234 AISI 4130 3000LB 45 Deg Threaded Elbow, Alloy Steel 45 Deg Threaded Elbow, Duplex Steel 45 Deg Threaded Elbow, Nickel Alloy 45 Deg Threaded Elbow Manufacturer in Mumbai, India.
Shikhar Steel is a prominent leader in Supplier & Exporter of 45 Degree Threaded Elbow in India. Forged Threaded 45 Deg Elbows are used in different industries applications like chemical processing, oil refineries, petrochemical and many other industries.Threaded 45° Pipe Elbows to join pipe to fittings or to other sections of pipe. We also supply 45 Degree Threaded Elbow in in customized size. Elbows are industrial fittings that change the direction of piping. Stainless Steel Threaded / Screwed 45° Elbows are defined as a part of the pipe fitting system. Sometimes, it is referred to as street eighth elbow. These Threaded Elbows make 45° changes of direction in the run of the pipe. It comes in two types; Short Radius Elbow and Long Radius Elbow.
Our offered range of ASME B16.11 / BS3799 Threaded 45 Deg Elbow is known for their low maintenance, weather resistance, high strength, easy to install and strong construction and are available in various diameters and at market leading price.
BS3799 45 Deg Threaded Elbow, Inconel 45 Deg Threaded Elbow, Monel 45 Deg Threaded Elbow, Hastelloy 45 Deg Threaded Elbow, Alloy 20 45 Deg Threaded Elbow, Copper Nickel 45 Deg Threaded Elbow, Titanium 45 Deg Threaded Elbow, 6000LB 45 Deg Threaded Elbow Suppliers in India.
Key Charactristic:
- Corrosion resistance
- Resistance to oxidation and sulfidation
- Cryogenic strength
- Resistance to abrasion and erosion
- Surface finish
- Magnetic properties
- Ductility
- Elevated temperature strength
- Stability of properties in service
- Suitability for intended fabrication techniques
Threaded 45 Degree Elbow Specifications
| Fittings | Threaded 45 Deg Elbow |
| Standard | ASME A182, ASME B16.9, ASME B16.11, MSS SP-43, MSS SP-95, BS3799 |
| Dimension | ASME 16.11, MSS SP-79, 83, 95, 97, BS 3799 |
| Size | 1/8″~4″ (DN6~DN100) |
| Class | 2000 LBS, 3000 LBS, 6000 LBS, 9000 LBS |
| Form | Forged Elbow, Screwed 90 Deg Elbow. |
Threaded 45 Degree Elbow Material & Grades
| Stainless Steel Threaded 45 Deg Elbow |
ASTM A182 F304, F304L, F306, F316L, F304H, F309S, F309H, F310S, F310H, F316TI, F316H, F316LN, F317, F317L, F321, F321H, F11, F22, F91, F347, F347H, F904L, ASTM A312/A403 TP304, TP304L, TP316, TP316L |
| Alloy Steel Threaded 45 Deg Elbow |
ASTM / ASME A 182, ASTM / ASME A 335, ASTM / ASME A 234 GR P 1, P 5, P 9, P 11, P 12, P 22, P 23, P 91, ASTM / ASME A 691 GR 1 CR, 1 1/4 CR, 2 1/4 CR, 5 CR, 9CR, 91 |
| Carbon Steel Threaded 45 Deg Elbow |
ASTM/ ASME A 105, ASTM/ ASME A 350 LF 2, ASTM / ASME A 53 GR. A & B, ASTM A 106 GR. A, B & C. API 5L GR. B, API 5L X 42, X 46, X 52, X 60, X 65 & X 70. ASTM / ASME A 691 GR A, B & C |
| Copper Alloy Threaded 45 Deg Elbow |
ASTM / ASME SB 111 UNS NO. C 10100 , C 10200 , C 10300 , C 10800 , C 12000, C 12200, C 70600 C 71500, ASTM / ASME SB 466 UNS NO. C 70600 ( CU -NI- 90/10) , C 71500 ( CU -NI- 70/30) |
| Nickel Alloy Threaded 45 Deg Elbow |
ASTM / ASME SB 336, ASTM / ASME SB 564 / 160 / 163 / 472, UNS 2200 (NICKEL 200) , UNS 2201 (NICKEL 201 ) , UNS 4400 (MONEL 400 ) , UNS 8020 ( ALLOY 20 / 20 CB 3 ) , UNS 8825 INCONEL (825) , UNS 6600 (INCONEL 600 ) , UNS 6601 (INCONEL 601) , UNS 6625 (INCONEL 625) , UNS 10276 (HASTELLOY C 276) |
| Duplex Stainless Steel Threaded 45 Deg Elbow |
ASTM / ASME A/SA 182 UNS F 44, F 45, F51, F 53, F 55, F 60, F 61. |
Dimensions of Threaded Elbow 45° - NPS 1/2 to 4 - 2000 LBS - ASME B16.11
| NPS | Minimum Length of Thread |
Outside Diameter of Band |
Minimum Wall Thickness |
Center to End | ||
| B | J | D | G | 90° A |
45° C |
|
| 1/2 | 10.9 | 13.6 | 33 | 3.18 | 28 | 22 |
| 3/4 | 12.7 | 13.9 | 38 | 3.18 | 33 | 25 |
| 1 | 14.7 | 17.3 | 46 | 3.68 | 38 | 28 |
| 1¼ | 17 | 18 | 56 | 3.89 | 44 | 33 |
| 1½ | 17.8 | 18.4 | 62 | 4.01 | 51 | 35 |
| 2 | 19 | 19.2 | 75 | 4.27 | 60 | 43 |
| 2½ | 23.6 | 28.9 | 92 | 5.61 | 76 | 52 |
| 3 | 25.9 | 30.5 | 109 | 5.99 | 86 | 64 |
| 4 | 27.7 | 33 | 146 | 6.55 | 106 | 79 |
Dimensions of Threaded Elbow 45° - NPS 1/2 to 4 - 3000 LBS- ASME B16.11
| NPS | Minimum Length of Thread |
Outside Diameter of Band |
Minimum Wall Thickness |
Center to End | ||
| B | J | D | G | 90° A |
45° C |
|
| 1/2 | 10.9 | 13.6 | 38 | 4.09 | 33 | 25 |
| 3/4 | 12.7 | 13.9 | 46 | 4.32 | 38 | 28 |
| 1 | 14.7 | 17.3 | 56 | 4.98 | 44 | 33 |
| 1¼ | 17 | 18 | 62 | 5.28 | 51 | 35 |
| 1½ | 17.8 | 18.4 | 75 | 5.56 | 60 | 43 |
| 2 | 19 | 19.2 | 84 | 7.14 | 64 | 44 |
| 2½ | 23.6 | 28.9 | 102 | 7.65 | 83 | 52 |
| 3 | 25.9 | 30.5 | 121 | 8.84 | 95 | 64 |
| 4 | 27.7 | 33 | 152 | 11.18 | 114 | 79 |
Dmensions of Threaded Elbow 45° - NPS 1/2 to 4 - 6000 LBS - ASME B16.11
| NPS | Minimum Length of Thread |
Outside Diameter of Band |
Minimum Wall Thickness |
Center to End | ||
| B | J | D | G | 90° A |
45° C |
|
| 1/2 | 10.9 | 13.6 | 46 | 8.15 | 38 | 28 |
| 3/4 | 12.7 | 13.9 | 56 | 8.53 | 44 | 33 |
| 1 | 14.7 | 17.3 | 62 | 9.93 | 51 | 35 |
| 1¼ | 17 | 18 | 75 | 10.59 | 60 | 43 |
| 1½ | 17.8 | 18.4 | 84 | 11.07 | 64 | 44 |
| 2 | 19 | 19.2 | 102 | 12.09 | 83 | 52 |
| 2½ | 23.6 | 28.9 | 121 | 15.29 | 95 | 64 |
| 3 | 25.9 | 30.5 | 146 | 16.64 | 106 | 79 |
| 4 | 27.7 | 33 | 152 | 18.67 | 114 | 79 |
Other Types of Threaded 45 Degree Elbow
- SS 45 Deg Threaded Elbow Supplier in UAE
- Stainless Steel 45 Deg Threaded Elbow Manufacturer in India
- ASME B16.11 45 Deg Threaded Elbow
- Carbon Steel 45 Deg Threaded Elbow
- Alloy Steel 45 Deg Threaded Elbow
- Duplex Steel 45 Deg Threaded Elbow
- ANSI B16.9 45 Deg Threaded Elbow Distributors
- Nickel Alloy 45 Deg Threaded Elbow
- ASME A182 6000LB 45 Deg Threaded Elbow
- Titanium 45 Deg Threaded Elbow
- Nickel 45 Deg Threaded Elbow
- Inconel 45 Deg Threaded Elbow Supplier in Poland
- Stainless Steel 45 Deg Threaded Elbow
- Carbon Steel 45 Deg Threaded Elbow in Qatar
- Duplex Steel 45 Deg Threaded Elbow
- Hastelloy 45 Deg Threaded Elbow
- Alloy 20 45 Deg Threaded Elbow
- Alloy Steel 45 Deg Threaded Elbow
- Copper Nickel 45 Deg Threaded Elbow
Countries We Export to
Nickel Super Alloys manufactures and exports Threaded 45 Degree Elbow to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia
Cities We Deliver to
Nickel Super Alloys manufactures and exports Threaded 45 Degree Elbow to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo