Stainless Steel 310 / 310S Flanges
ASME SA182 SS F310 Industrial Flanges, UNS S31008 SS WNRF Flanges, ANSI B16.5 SS 310 Orifice Flange, SS 310 Nippo Flanges, SS UNS S31000 Pipe Flanges, Stainless Steel 310S RTJ Flange Manufacturer in Mumbai,India.
Nickel Super Alloys is a prominent firm in manufacturing an exporting Stainless Steel 310 / 310S Flanges, which is often used at cryogenic temperatures. Stainless Steel 310 Slip On Raised Flanges is used along with hot acetic and citric acid in the food processing industry. Stainless Steel 310S Blind Raised Flanges is recommended that this steel should not be continuously used at 797 Degree F – 1580 Degree F range due to carbide precipitation. Fusion point is lower than that of non-alloyed steels, and so austenitic Stainless Steel 310 Spectacle Blind Flanges have to be welded with lower heat input than non-alloyed steels. Stainless Steel 310S Threaded Flanges are austenitic, resulting in relatively high creep strength values.
Stainless Steel 310 Socket Weld Flanges is utilized for ease of fabrication due to its better formability and weldability. Stainless Steel 310S Weld Neck Flanges is often used in kiln liners, auto exhaust parts, and boiler baffles. Stainless Steel 310 Lap Joint Flanges has oxidation resistance to 2000 Degree F. Stainless Steel 310S Ring Joint TypeFlanges finds usage in cryogenic applications with low magnetic permeability. Stainless Steel 310 Nippolet Flanges is also used in muffles, retorts, andannealing covers. Stainless Steel UNS S31000 Flanges is used widely in industries such as heat treatment and chemical processing. Stainless Steel UNS S31008 Flanges is also very ductile, and has good weldability enabling its widespread usage in many applications.
Stainless Steel 310 Pipe Flanges, Stainless Steel 310 Nippolet Flanges, SS 310S Weld Neck Flange, SS 310 Slip On Flanges, SS 310 Lap Joint Flange, SS DIN 1.4841, 1.4845 Socket Weld Flanges, ASTM A182 SS F310 Threaded Flanges Suppliers in India.
Key Charactristic:
- Corrosion resistance
- Resistance to oxidation and sulfidation
- Cryogenic strength
- Resistance to abrasion and erosion
- Surface finish
- Magnetic properties
- Ductility
- Elevated temperature strength
- Stability of properties in service
- Suitability for intended fabrication techniques
Stainless Steel 310 / 310S Specifications
| Grade | Stainless Steel 310/310S | SS 310/310S | UNS S31000/S31008 |
| Standard | ASTM A182, ASME SA182 |
| Dimensions | ANSI / ASME B16.5, B16.47 Series A & B, B.16.48, BS4504, BS10, DIN, EN-1092, MSS SP44 |
| Size | 1/2" - 48" (15NB - 1200NB) |
| Class / Pressure Rating | 150 Class, 300 Class, 718 Class, 900 Class, 1500 Class, 2500 Class, PN6, PN10, PN16, PN25, PN40, PN64, etc. |
| Form | Slip on Flanges (SORF), Threaded Flanges, Weld neck Flanges (WNRF), Blind Flanges, Socket weld Flanges, Lap Joint Flanges, Ring Type Joint Flanges, Spectacle Blind Flanges, Spacer Ring Flanges, Long weld Neck Flanges, Nipo Flange, Nipolet Flanges, Plate Flanges, Flat Flange, Orifice Flanges, Forged Flanges |
| Flange Face Type | Flat Face (FF), Raised Face (RF), Ring Type Joint(RTJ) |
| STANDARD | WERKSTOFF NR. | UNS | JIS | BS | GOST | AFNOR | EN |
| SS 310 | 1.4841 | S31000 | SUS 310 | 310S24 | 20Ch25N20S2 | – | X15CrNi25-20 |
| SS 310S | 1.4845 | S31008 | SUS 310S | 310S16 | 20Ch23N18 | – | X8CrNi25-21 |
Stainless Steel 310 / 310S Flanges Chemical Composition
| Grade | C | Mn | Si | P | S | Cr | Mo | Ni | N |
| SS 310 | 0.015 max | 2 max | 0.015 max | 0.020 max | 0.015 max | 24.00 – 26.00 | 0.10 max | 19.00 – 21.00 | 54.7 min |
| SS 310S | 0.08 max | 2 max | 1.00 max | 0.045 max | 0.030 max | 24.00 – 26.00 | 0.75 max | 19.00 – 21.00 | 53.095 min |
Stainless Steel 30 / 310S Flanges Mechanical Properties
| Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
| 7.9 g/cm3 | 1402 °C (2555 °F)s | Psi – 75000 , MPa – 515 | Psi – 30000 , MPa – 205 | 40 % |
Other Types of Stainless Steel 310 / 310S Flanges
- DIN 1.4841 / 1.4845 Tongue & Groove Flanges Supplier in UAE
- SS 310 Spectacle blind flanges Manufacturer in India
- SUS 310S Long Weld Neck Flanges
- DIN 1.4841 / 1.4845 Flat Face Flanges
- UNS S31000 High Hub Blind Flanges
- DIN 1.4841 Lap Joint Flanges
- DIN 1.4845 Reducing Flanges Distributors
- UNS S31008 Blind Flanges
- ASME SA182 UNS S31000 Slip On Flanges
- Stainless Steel 310S Threaded Flanges
- ASME SA182 SS 310 Orifice Flanges Exporter in Russia
- SS 310S Forged Flanges
- UNS S31000 SS 310 Plate Flanges Supplier in Poland
- SS 310S Spacer Ring Flanges
- SS 310S Nipo Flange in Qatar
- UNS S31000 / S31008 Nipolet Flanges
- 310 Stainless Steel Pipe Flanges
- SS 310S SORF Flanges
- ASTM A182 SS 310S WNRF Flanges
- UNS S31000 / S31008 Threaded Flanges
Countries We Export to
Nickel Super Alloys manufactures and exports Stainless Steel 310 / 310S Flanges to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia
Cities We Deliver to
Nickel Super Alloys manufactures and exports Stainless Steel 310 / 310S Flanges to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo